{"id":5620,"date":"2025-03-01T13:00:00","date_gmt":"2025-03-01T06:00:00","guid":{"rendered":"https:\/\/hoachatlocthien.com\/?p=5620"},"modified":"2025-07-17T15:27:15","modified_gmt":"2025-07-17T08:27:15","slug":"thuy-tinh-long-la-gi","status":"publish","type":"post","link":"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi","title":{"rendered":"Th\u1ee7y Tinh L\u1ecfng (Natri Silicat) &#8211; \u1ee8ng D\u1ee5ng Trong S\u1ea3n Xu\u1ea5t C\u00f4ng Nghi\u1ec7p"},"content":{"rendered":"<p data-start=\"65\" data-end=\"490\">Trong nhi\u1ec1u ng\u00e0nh c\u00f4ng nghi\u1ec7p, t\u1eeb x\u00e2y d\u1ef1ng, x\u1eed l\u00fd n\u01b0\u1edbc, \u0111\u1ebfn s\u1ea3n xu\u1ea5t gi\u1ea5y, d\u1ec7t nhu\u1ed9m v\u00e0 keo d\u00e1n, th\u1ee7y tinh l\u1ecfng (Natri Silicat &#8211; Na\u2082SiO\u2083) \u0111\u00f3ng vai tr\u00f2 quan tr\u1ecdng nh\u1edd v\u00e0o kh\u1ea3 n\u0103ng k\u1ebft d\u00ednh m\u1ea1nh, ch\u1ed1ng th\u1ea5m hi\u1ec7u qu\u1ea3 v\u00e0 ch\u1ecbu nhi\u1ec7t t\u1ed1t. Kh\u00f4ng ch\u1ec9 gi\u00fap gia c\u1ed1 v\u1eadt li\u1ec7u v\u00e0 t\u1ed1i \u01b0u h\u00f3a quy tr\u00ecnh s\u1ea3n xu\u1ea5t, keo th\u1ee7y tinh l\u1ecfng c\u00f2n \u0111\u01b0\u1ee3c \u1ee9ng d\u1ee5ng r\u1ed9ng r\u00e3i trong ch\u1ed1ng ch\u00e1y, \u1ed5n \u0111\u1ecbnh pH v\u00e0 b\u1ea3o v\u1ec7 b\u1ec1 m\u1eb7t kim lo\u1ea1i.<\/p>\r\n<p data-start=\"492\" data-end=\"733\">V\u1eady th\u1ee7y tinh l\u1ecfng l\u00e0 g\u00ec? T\u1ea1i sao h\u1ee3p ch\u1ea5t n\u00e0y l\u1ea1i \u0111\u01b0\u1ee3c s\u1eed d\u1ee5ng ph\u1ed5 bi\u1ebfn trong nhi\u1ec1u l\u0129nh v\u1ef1c s\u1ea3n xu\u1ea5t? H\u00e3y c\u00f9ng H\u00f3a Ch\u1ea5t L\u1ed9c Thi\u00ean kh\u00e1m ph\u00e1 nh\u1eefng \u1ee9ng d\u1ee5ng th\u1ef1c t\u1ebf v\u00e0 l\u1ee3i \u00edch v\u01b0\u1ee3t tr\u1ed9i c\u1ee7a Natri Silicat trong b\u00e0i vi\u1ebft d\u01b0\u1edbi \u0111\u00e2y.<\/p>\r\n<div id=\"ez-toc-container\" class=\"ez-toc-v2_0_72 counter-hierarchy ez-toc-counter ez-toc-grey ez-toc-container-direction\">\n<div class=\"ez-toc-title-container\">\n<p class=\"ez-toc-title\" style=\"cursor:inherit\">N\u1ed9i dung<\/p>\n<span class=\"ez-toc-title-toggle\"><a href=\"#\" class=\"ez-toc-pull-right ez-toc-btn ez-toc-btn-xs ez-toc-btn-default ez-toc-toggle\" aria-label=\"Toggle Table of Content\"><span class=\"ez-toc-js-icon-con\"><span class=\"\"><span class=\"eztoc-hide\" style=\"display:none;\">Toggle<\/span><span class=\"ez-toc-icon-toggle-span\"><svg style=\"fill: #dd3333;color:#dd3333\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\" class=\"list-377408\" width=\"20px\" height=\"20px\" viewbox=\"0 0 24 24\" fill=\"none\"><path d=\"M6 6H4v2h2V6zm14 0H8v2h12V6zM4 11h2v2H4v-2zm16 0H8v2h12v-2zM4 16h2v2H4v-2zm16 0H8v2h12v-2z\" fill=\"currentColor\"><\/path><\/svg><svg style=\"fill: #dd3333;color:#dd3333\" class=\"arrow-unsorted-368013\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\" width=\"10px\" height=\"10px\" viewbox=\"0 0 24 24\" version=\"1.2\" baseprofile=\"tiny\"><path d=\"M18.2 9.3l-6.2-6.3-6.2 6.3c-.2.2-.3.4-.3.7s.1.5.3.7c.2.2.4.3.7.3h11c.3 0 .5-.1.7-.3.2-.2.3-.5.3-.7s-.1-.5-.3-.7zM5.8 14.7l6.2 6.3 6.2-6.3c.2-.2.3-.5.3-.7s-.1-.5-.3-.7c-.2-.2-.4-.3-.7-.3h-11c-.3 0-.5.1-.7.3-.2.2-.3.5-.3.7s.1.5.3.7z\"\/><\/svg><\/span><\/span><\/span><\/a><\/span><\/div>\n<nav><ul class='ez-toc-list ez-toc-list-level-1' ><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-1\" href=\"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi\/#Thuy_tinh_long_la_gi\" title=\"Th\u1ee7y tinh l\u1ecfng l\u00e0 g\u00ec?\">Th\u1ee7y tinh l\u1ecfng l\u00e0 g\u00ec?<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-2\" href=\"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi\/#Thanh_phan_Tinh_chat_cua_thuy_tinh_long\" title=\"Th\u00e0nh ph\u1ea7n &amp; T\u00ednh ch\u1ea5t c\u1ee7a th\u1ee7y tinh l\u1ecfng\">Th\u00e0nh ph\u1ea7n &amp; T\u00ednh ch\u1ea5t c\u1ee7a th\u1ee7y tinh l\u1ecfng<\/a><ul class='ez-toc-list-level-4' ><li class='ez-toc-heading-level-4'><ul class='ez-toc-list-level-4' ><li class='ez-toc-heading-level-4'><a class=\"ez-toc-link ez-toc-heading-3\" href=\"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi\/#Mot_so_luu_y_ve_tinh_chat_cua_thuy_tinh_long\" title=\"M\u1ed9t s\u1ed1 l\u01b0u \u00fd v\u1ec1 t\u00ednh ch\u1ea5t c\u1ee7a th\u1ee7y tinh l\u1ecfng:\">M\u1ed9t s\u1ed1 l\u01b0u \u00fd v\u1ec1 t\u00ednh ch\u1ea5t c\u1ee7a th\u1ee7y tinh l\u1ecfng:<\/a><\/li><\/ul><\/li><li class='ez-toc-page-1 ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-4\" href=\"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi\/#Natri_Silicat_va_Kali_Silicat_%E2%80%93_Diem_khac_biet\" title=\"Natri Silicat v\u00e0 Kali Silicat \u2013 \u0110i\u1ec3m kh\u00e1c bi\u1ec7t\">Natri Silicat v\u00e0 Kali Silicat \u2013 \u0110i\u1ec3m kh\u00e1c bi\u1ec7t<\/a><\/li><\/ul><\/li><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-5\" href=\"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi\/#Ung_dung_cua_thuy_tinh_long_trong_cong_nghiep\" title=\"\u1ee8ng d\u1ee5ng c\u1ee7a th\u1ee7y tinh l\u1ecfng trong c\u00f4ng nghi\u1ec7p\">\u1ee8ng d\u1ee5ng c\u1ee7a th\u1ee7y tinh l\u1ecfng trong c\u00f4ng nghi\u1ec7p<\/a><ul class='ez-toc-list-level-3' ><li class='ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-6\" href=\"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi\/#Nganh_xay_dung_%E2%80%93_Chong_tham_gia_co_be_tong_tang_do_ben_vat_lieu\" title=\"Ng\u00e0nh x\u00e2y d\u1ef1ng &#8211; Ch\u1ed1ng th\u1ea5m, gia c\u1ed1 b\u00ea t\u00f4ng, t\u0103ng \u0111\u1ed9 b\u1ec1n v\u1eadt li\u1ec7u\">Ng\u00e0nh x\u00e2y d\u1ef1ng &#8211; Ch\u1ed1ng th\u1ea5m, gia c\u1ed1 b\u00ea t\u00f4ng, t\u0103ng \u0111\u1ed9 b\u1ec1n v\u1eadt li\u1ec7u<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-7\" href=\"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi\/#Nganh_xu_ly_nuoc_%E2%80%93_Keo_tu_on_dinh_pH_loai_bo_kim_loai_nang\" title=\"Ng\u00e0nh x\u1eed l\u00fd n\u01b0\u1edbc &#8211; Keo t\u1ee5, \u1ed5n \u0111\u1ecbnh pH, lo\u1ea1i b\u1ecf kim lo\u1ea1i n\u1eb7ng\">Ng\u00e0nh x\u1eed l\u00fd n\u01b0\u1edbc &#8211; Keo t\u1ee5, \u1ed5n \u0111\u1ecbnh pH, lo\u1ea1i b\u1ecf kim lo\u1ea1i n\u1eb7ng<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-8\" href=\"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi\/#Nganh_det_nhuom_%E2%80%93_On_dinh_mau_vai_chong_chay\" title=\"Ng\u00e0nh d\u1ec7t nhu\u1ed9m &#8211; \u1ed4n \u0111\u1ecbnh m\u00e0u v\u1ea3i, ch\u1ed1ng ch\u00e1y\">Ng\u00e0nh d\u1ec7t nhu\u1ed9m &#8211; \u1ed4n \u0111\u1ecbnh m\u00e0u v\u1ea3i, ch\u1ed1ng ch\u00e1y<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-9\" href=\"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi\/#Nganh_san_xuat_giay_%E2%80%93_Gia_co_be_mat_tang_do_ben_va_chong_am\" title=\"Ng\u00e0nh s\u1ea3n xu\u1ea5t gi\u1ea5y &#8211; Gia c\u1ed1 b\u1ec1 m\u1eb7t, t\u0103ng \u0111\u1ed9 b\u1ec1n v\u00e0 ch\u1ed1ng \u1ea9m\">Ng\u00e0nh s\u1ea3n xu\u1ea5t gi\u1ea5y &#8211; Gia c\u1ed1 b\u1ec1 m\u1eb7t, t\u0103ng \u0111\u1ed9 b\u1ec1n v\u00e0 ch\u1ed1ng \u1ea9m<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-10\" href=\"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi\/#Nganh_san_xuat_keo_dan_cong_nghiep_%E2%80%93_Chat_ket_dinh_ben_vung\" title=\"Ng\u00e0nh s\u1ea3n xu\u1ea5t keo d\u00e1n c\u00f4ng nghi\u1ec7p &#8211; Ch\u1ea5t k\u1ebft d\u00ednh b\u1ec1n v\u1eefng\">Ng\u00e0nh s\u1ea3n xu\u1ea5t keo d\u00e1n c\u00f4ng nghi\u1ec7p &#8211; Ch\u1ea5t k\u1ebft d\u00ednh b\u1ec1n v\u1eefng<\/a><\/li><\/ul><\/li><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-11\" href=\"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi\/#Huong_dan_bao_quan_Luu_y_khi_su_dung\" title=\"H\u01b0\u1edbng d\u1eabn b\u1ea3o qu\u1ea3n &amp; L\u01b0u \u00fd khi s\u1eed d\u1ee5ng\">H\u01b0\u1edbng d\u1eabn b\u1ea3o qu\u1ea3n &amp; L\u01b0u \u00fd khi s\u1eed d\u1ee5ng<\/a><ul class='ez-toc-list-level-3' ><li class='ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-12\" href=\"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi\/#Cach_bao_quan\" title=\"C\u00e1ch b\u1ea3o qu\u1ea3n\">C\u00e1ch b\u1ea3o qu\u1ea3n<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-13\" href=\"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi\/#Luu_y_an_toan\" title=\"L\u01b0u \u00fd an to\u00e0n\">L\u01b0u \u00fd an to\u00e0n<\/a><\/li><\/ul><\/li><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-14\" href=\"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi\/#Lien_he_dat_hang_thuy_tinh_long_tai_Loc_Thien\" title=\"Li\u00ean h\u1ec7 \u0111\u1eb7t h\u00e0ng th\u1ee7y tinh l\u1ecfng t\u1ea1i L\u1ed9c Thi\u00ean\">Li\u00ean h\u1ec7 \u0111\u1eb7t h\u00e0ng th\u1ee7y tinh l\u1ecfng t\u1ea1i L\u1ed9c Thi\u00ean<\/a><ul class='ez-toc-list-level-3' ><li class='ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-15\" href=\"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi\/#Thuy_tinh_long_co_an_toan_cho_con_nguoi_khong\" title=\"Th\u1ee7y tinh l\u1ecfng c\u00f3 an to\u00e0n cho con ng\u01b0\u1eddi kh\u00f4ng?\">Th\u1ee7y tinh l\u1ecfng c\u00f3 an to\u00e0n cho con ng\u01b0\u1eddi kh\u00f4ng?<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-16\" href=\"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi\/#Thuy_tinh_long_co_the_su_dung_trong_san_xuat_gom_su_khong\" title=\"Th\u1ee7y tinh l\u1ecfng c\u00f3 th\u1ec3 s\u1eed d\u1ee5ng trong s\u1ea3n xu\u1ea5t g\u1ed1m s\u1ee9 kh\u00f4ng?\">Th\u1ee7y tinh l\u1ecfng c\u00f3 th\u1ec3 s\u1eed d\u1ee5ng trong s\u1ea3n xu\u1ea5t g\u1ed1m s\u1ee9 kh\u00f4ng?<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-17\" href=\"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi\/#Thuy_tinh_long_co_the_tai_su_dung_khong\" title=\"Th\u1ee7y tinh l\u1ecfng c\u00f3 th\u1ec3 t\u00e1i s\u1eed d\u1ee5ng kh\u00f4ng?\">Th\u1ee7y tinh l\u1ecfng c\u00f3 th\u1ec3 t\u00e1i s\u1eed d\u1ee5ng kh\u00f4ng?<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-18\" href=\"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi\/#Thuy_tinh_long_co_bi_dong_cung_khong_Cach_khac_phuc_khi_bi_dong_dac\" title=\"Th\u1ee7y tinh l\u1ecfng c\u00f3 b\u1ecb \u0111\u00f4ng c\u1ee9ng kh\u00f4ng? C\u00e1ch kh\u1eafc ph\u1ee5c khi b\u1ecb \u0111\u00f4ng \u0111\u1eb7c?\">Th\u1ee7y tinh l\u1ecfng c\u00f3 b\u1ecb \u0111\u00f4ng c\u1ee9ng kh\u00f4ng? C\u00e1ch kh\u1eafc ph\u1ee5c khi b\u1ecb \u0111\u00f4ng \u0111\u1eb7c?<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-19\" href=\"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi\/#Thuy_tinh_long_co_bi_dong_cung_khong_Cach_khac_phuc_khi_bi_dong_dac-2\" title=\"Th\u1ee7y tinh l\u1ecfng c\u00f3 b\u1ecb \u0111\u00f4ng c\u1ee9ng kh\u00f4ng? C\u00e1ch kh\u1eafc ph\u1ee5c khi b\u1ecb \u0111\u00f4ng \u0111\u1eb7c?\">Th\u1ee7y tinh l\u1ecfng c\u00f3 b\u1ecb \u0111\u00f4ng c\u1ee9ng kh\u00f4ng? C\u00e1ch kh\u1eafc ph\u1ee5c khi b\u1ecb \u0111\u00f4ng \u0111\u1eb7c?<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-3'><a class=\"ez-toc-link ez-toc-heading-20\" href=\"https:\/\/hoachatlocthien.com\/ko\/thuy-tinh-long-la-gi\/#Thuy_tinh_long_co_anh_huong_den_moi_truong_khong\" title=\"Th\u1ee7y tinh l\u1ecfng c\u00f3 \u1ea3nh h\u01b0\u1edfng \u0111\u1ebfn m\u00f4i tr\u01b0\u1eddng kh\u00f4ng?\">Th\u1ee7y tinh l\u1ecfng c\u00f3 \u1ea3nh h\u01b0\u1edfng \u0111\u1ebfn m\u00f4i tr\u01b0\u1eddng kh\u00f4ng?<\/a><\/li><\/ul><\/li><\/ul><\/nav><\/div>\n<h2 class=\"wp-block-heading\"><span class=\"ez-toc-section\" id=\"Thuy_tinh_long_la_gi\"><\/span><span style=\"font-weight: 400;\"><strong>Th\u1ee7y tinh l\u1ecfng l\u00e0 g\u00ec?<\/strong><\/span><span class=\"ez-toc-section-end\"><\/span><\/h2><p><span style=\"font-weight: 400;\">Th\u1ee7y tinh l\u1ecfng l\u00e0 g\u00ec? <\/span>Th\u1ee7y tinh l\u1ecfng, hay c\u00f2n g\u1ecdi l\u00e0 Sodium Silicate ho\u1eb7c Water Glass trong ti\u1ebfng Anh, l\u00e0 m\u1ed9t dung d\u1ecbch \u0111\u1eb7c c\u1ee7a Natri Silicat (Na\u2082SiO\u2083) v\u00e0 \u0111\u00f4i khi c\u00f3 th\u00eam Kali Silicat (K\u2082SiO\u2083) t\u00f9y theo m\u1ee5c \u0111\u00edch s\u1eed d\u1ee5ng. \u0110\u00e2y l\u00e0 m\u1ed9t h\u1ee3p ch\u1ea5t silicat ki\u1ec1m c\u00f3 \u0111\u1ed9 nh\u1edbt cao, trong su\u1ed1t ho\u1eb7c h\u01a1i v\u00e0ng, d\u1ec5 h\u00f2a tan trong n\u01b0\u1edbc v\u00e0 c\u00f3 t\u00ednh ki\u1ec1m m\u1ea1nh.<\/p>\r\n<ul>\r\n<li>C\u00f4ng th\u1ee9c h\u00f3a h\u1ecdc t\u1ed5ng qu\u00e1t c\u1ee7a th\u1ee7y tinh l\u1ecfng l\u00e0 mNa\u2082O\u00b7nSiO\u2082, trong \u0111\u00f3 m v\u00e0 n thay \u0111\u1ed5i t\u00f9y theo t\u1ef7 l\u1ec7 Na\u2082O v\u00e0 SiO\u2082, quy\u1ebft \u0111\u1ecbnh c\u00e1c t\u00ednh ch\u1ea5t v\u1eadt l\u00fd v\u00e0 h\u00f3a h\u1ecdc c\u1ee7a dung d\u1ecbch.<\/li>\r\n<li>Nh\u1edd kh\u1ea3 n\u0103ng k\u1ebft d\u00ednh t\u1ed1t, ch\u1ecbu nhi\u1ec7t cao v\u00e0 ch\u1ed1ng th\u1ea5m hi\u1ec7u qu\u1ea3, th\u1ee7y tinh l\u1ecfng \u0111\u01b0\u1ee3c \u1ee9ng d\u1ee5ng r\u1ed9ng r\u00e3i trong c\u00e1c ng\u00e0nh x\u00e2y d\u1ef1ng, x\u1eed l\u00fd n\u01b0\u1edbc, d\u1ec7t nhu\u1ed9m, s\u1ea3n xu\u1ea5t gi\u1ea5y, xi m\u1ea1 v\u00e0 keo d\u00e1n c\u00f4ng nghi\u1ec7p.<\/li>\r\n<\/ul><p><span style=\"font-weight: 400;\">B\u1ea1n \u0111ang c\u1ea7n mua th\u1ee7y tinh l\u1ecfng ch\u1ea5t l\u01b0\u1ee3ng cao? Li\u00ean h\u1ec7 ngay H\u00f3a Ch\u1ea5t L\u1ed9c Thi\u00ean \u0111\u1ec3 nh\u1eadn b\u00e1o gi\u00e1 t\u1ed1t nh\u1ea5t!\u00a0<\/span><\/p><h2 class=\"wp-block-heading\"><span class=\"ez-toc-section\" id=\"Thanh_phan_Tinh_chat_cua_thuy_tinh_long\"><\/span><span style=\"font-weight: 400;\"><strong>Th\u00e0nh ph\u1ea7n &amp; T\u00ednh ch\u1ea5t c\u1ee7a th\u1ee7y tinh l\u1ecfng<\/strong><\/span><span class=\"ez-toc-section-end\"><\/span><\/h2><p data-start=\"1821\" data-end=\"1962\">Th\u1ee7y tinh l\u1ecfng ch\u1ee7 y\u1ebfu l\u00e0 dung d\u1ecbch \u0111\u1eb7c c\u1ee7a <strong data-start=\"1865\" data-end=\"1892\">Natri Silicat (Na\u2082SiO\u2083)<\/strong> v\u00e0 \u0111\u00f4i khi c\u00f3 th\u00eam <strong data-start=\"1912\" data-end=\"1937\">Kali Silicat (K\u2082SiO\u2083)<\/strong>. Th\u00e0nh ph\u1ea7n ch\u00ednh g\u1ed3m:<\/p>\r\n<ul data-start=\"1963\" data-end=\"2176\">\r\n<li data-start=\"1963\" data-end=\"2101\"><strong data-start=\"1965\" data-end=\"1986\">Natri Oxit (Na\u2082O)<\/strong> \uadf8\ub9ac\uace0 <strong data-start=\"1990\" data-end=\"2013\">Silic \u0110i\u00f4x\u00edt (SiO\u2082)<\/strong> theo t\u1ef7 l\u1ec7 kh\u00e1c nhau, quy\u1ebft \u0111\u1ecbnh t\u00ednh ch\u1ea5t k\u1ebft d\u00ednh, \u0111\u1ed9 b\u1ec1n v\u00e0 \u0111\u1ed9 nh\u1edbt c\u1ee7a dung d\u1ecbch.<\/li>\r\n<li data-start=\"2102\" data-end=\"2176\">C\u00f4ng th\u1ee9c t\u1ed5ng qu\u00e1t: <strong data-start=\"2125\" data-end=\"2140\">mNa\u2082O\u00b7nSiO\u2082<\/strong> (t\u00f9y thu\u1ed9c v\u00e0o t\u1ef7 l\u1ec7 th\u00e0nh ph\u1ea7n).<\/li>\r\n<\/ul>\r\n<figure id=\"attachment_5621\" aria-describedby=\"caption-attachment-5621\" style=\"width: 366px\" class=\"wp-caption aligncenter\"><img decoding=\"async\" class=\"wp-image-5621 lazyload\" data-src=\"https:\/\/hoachatlocthien.com\/wp-content\/uploads\/2025\/02\/Cong-thuc-hoa-hoc-Na\u2082SiO\u2083-png.webp\" alt=\"C\u00e1u tr\u00fac h\u00f3a h\u1ecdc c\u1ee7a Natri Silicat (Na\u2082SiO\u2083)\" width=\"366\" height=\"122\" src=\"data:image\/gif;base64,R0lGODlhAQABAAAAACH5BAEKAAEALAAAAAABAAEAAAICTAEAOw==\" style=\"--smush-placeholder-width: 366px; --smush-placeholder-aspect-ratio: 366\/122;\" \/><figcaption id=\"caption-attachment-5621\" class=\"wp-caption-text\">C\u00f4ng th\u1ee9c th\u1ee7y tinh l\u1ecfng Natri Silicat (Na\u2082SiO\u2083)<\/figcaption><\/figure>\r\n<figure class=\"wp-block-table\">\r\n<table data-start=\"2230\" data-end=\"2981\">\r\n<thead data-start=\"2230\" data-end=\"2300\">\r\n<tr data-start=\"2230\" data-end=\"2300\">\r\n<th data-start=\"2230\" data-end=\"2262\"><strong data-start=\"2232\" data-end=\"2245\">T\u00ednh ch\u1ea5t<\/strong><\/th>\r\n<th data-start=\"2262\" data-end=\"2300\"><strong data-start=\"2264\" data-end=\"2276\">\u0110\u1eb7c \u0111i\u1ec3m<\/strong><\/th>\r\n<\/tr>\r\n<\/thead>\r\n<tbody data-start=\"2368\" data-end=\"2981\">\r\n<tr data-start=\"2368\" data-end=\"2433\">\r\n<td><strong data-start=\"2370\" data-end=\"2391\">T\u00ean g\u1ecdi ti\u1ebfng Anh<\/strong><\/td>\r\n<td>Sodium Silicate, Water Glass<\/td>\r\n<\/tr>\r\n<tr data-start=\"2434\" data-end=\"2500\">\r\n<td><strong data-start=\"2436\" data-end=\"2457\">\ud654\ud559\uc2dd<\/strong><\/td>\r\n<td>Na\u2082SiO\u2083 ho\u1eb7c mNa\u2082O\u00b7nSiO\u2082<\/td>\r\n<\/tr>\r\n<tr data-start=\"2501\" data-end=\"2568\">\r\n<td><strong data-start=\"2503\" data-end=\"2517\">\uc0c1\ud0dc<\/strong><\/td>\r\n<td>Dung d\u1ecbch \u0111\u1eb7c, nh\u1edbt<\/td>\r\n<\/tr>\r\n<tr data-start=\"2569\" data-end=\"2636\">\r\n<td><strong data-start=\"2571\" data-end=\"2582\">M\u00e0u s\u1eafc<\/strong><\/td>\r\n<td>Trong su\u1ed1t ho\u1eb7c h\u01a1i v\u00e0ng<\/td>\r\n<\/tr>\r\n<tr data-start=\"2637\" data-end=\"2704\">\r\n<td><strong data-start=\"2639\" data-end=\"2648\">\u0110\u1ed9 pH<\/strong><\/td>\r\n<td>11-13 (t\u00ednh ki\u1ec1m m\u1ea1nh)<\/td>\r\n<\/tr>\r\n<tr data-start=\"2705\" data-end=\"2772\">\r\n<td><strong data-start=\"2707\" data-end=\"2719\">T\u1ef7 tr\u1ecdng<\/strong><\/td>\r\n<td>1,40 \u2013 1,42 g\/cm\u00b3<\/td>\r\n<\/tr>\r\n<tr data-start=\"2773\" data-end=\"2841\">\r\n<td><strong data-start=\"2775\" data-end=\"2789\">\uc6a9\ud574\ub3c4<\/strong><\/td>\r\n<td>H\u00f2a tan t\u1ed1t trong n\u01b0\u1edbc<\/td>\r\n<\/tr>\r\n<tr data-start=\"2842\" data-end=\"2910\">\r\n<td><strong data-start=\"2844\" data-end=\"2867\">Kh\u1ea3 n\u0103ng ch\u1ed1ng th\u1ea5m<\/strong><\/td>\r\n<td>Cao, t\u1ea1o l\u1edbp m\u00e0ng b\u1ea3o v\u1ec7 b\u1ec1 m\u1eb7t<\/td>\r\n<\/tr>\r\n<tr data-start=\"2911\" data-end=\"2981\">\r\n<td><strong data-start=\"2913\" data-end=\"2927\">Ch\u1ecbu nhi\u1ec7t<\/strong><\/td>\r\n<td>\u1ed4n \u0111\u1ecbnh trong \u0111i\u1ec1u ki\u1ec7n nhi\u1ec7t \u0111\u1ed9 cao<\/td>\r\n<\/tr>\r\n<\/tbody>\r\n<\/table>\r\n<\/figure><p><span style=\"font-weight: 400;\">Th\u1ee7y tinh l\u1ecfng c\u00f3 th\u1ec3 \u0111i\u1ec1u ch\u1ec9nh t\u1ef7 l\u1ec7 Na\u2082O\/SiO\u2082 \u0111\u1ec3 ph\u00f9 h\u1ee3p v\u1edbi t\u1eebng \u1ee9ng d\u1ee5ng c\u00f4ng nghi\u1ec7p kh\u00e1c nhau, gi\u00fap t\u0103ng c\u01b0\u1eddng kh\u1ea3 n\u0103ng k\u1ebft d\u00ednh, ch\u1ed1ng th\u1ea5m, ho\u1eb7c c\u1ea3i thi\u1ec7n t\u00ednh ch\u1ea5t c\u01a1 h\u1ecdc c\u1ee7a s\u1ea3n ph\u1ea9m.<\/span><\/p>\r\n<h4 data-start=\"2983\" data-end=\"3042\"><span class=\"ez-toc-section\" id=\"Mot_so_luu_y_ve_tinh_chat_cua_thuy_tinh_long\"><\/span><strong data-start=\"2988\" data-end=\"3040\">M\u1ed9t s\u1ed1 l\u01b0u \u00fd v\u1ec1 t\u00ednh ch\u1ea5t c\u1ee7a th\u1ee7y tinh l\u1ecfng:<\/strong><span class=\"ez-toc-section-end\"><\/span><\/h4>\r\n<ul data-start=\"3043\" data-end=\"3429\">\r\n<li data-start=\"3043\" data-end=\"3167\"><strong data-start=\"3045\" data-end=\"3071\">M\u1ee9c \u0111\u1ed9 &#8220;l\u1ecfng&#8221; v\u00e0 &#8220;\u0111\u1eb7c&#8221;<\/strong>: D\u00f9 \u0111\u01b0\u1ee3c g\u1ecdi l\u00e0 &#8220;th\u1ee7y tinh l\u1ecfng&#8221;, nh\u01b0ng th\u1ef1c ch\u1ea5t n\u00f3 l\u00e0 m\u1ed9t dung d\u1ecbch \u0111\u1eadm \u0111\u1eb7c c\u00f3 \u0111\u1ed9 nh\u1edbt cao.\r\n<ul data-start=\"3043\" data-end=\"3429\">\r\n<li data-start=\"3043\" data-end=\"3167\">V\u1eady c\u00f3 th\u1ec3 n\u00f3i r\u1eb1ng th\u1ee7y tinh l\u1ecfng l\u00e0 dung d\u1ecbch \u0111\u1eb7c c\u1ee7a <strong>c\u00e1c h\u1ee3p ch\u1ea5t silicat ki\u1ec1m, ch\u1ee7 y\u1ebfu l\u00e0 Natri Silicat (Na\u2082SiO\u2083) v\u00e0 \u0111\u00f4i khi c\u00f3 th\u00eam Kali Silicat (K\u2082SiO\u2083), v\u1edbi t\u1ef7 l\u1ec7 Na\u2082O\/SiO\u2082 \u0111\u01b0\u1ee3c \u0111i\u1ec1u ch\u1ec9nh \u0111\u1ec3 ph\u00f9 h\u1ee3p v\u1edbi t\u1eebng \u1ee9ng d\u1ee5ng c\u00f4ng nghi\u1ec7p.<\/strong><\/li>\r\n<\/ul>\r\n<\/li>\r\n<li data-start=\"3168\" data-end=\"3290\"><strong data-start=\"3170\" data-end=\"3184\">Ph\u1ea1m vi pH<\/strong>: Dung d\u1ecbch silicat ki\u1ec1m c\u00f3 pH <strong data-start=\"3215\" data-end=\"3227\">t\u1eeb 11-13<\/strong>, kh\u00f4ng c\u1ed1 \u0111\u1ecbnh \u1edf 11-12, ph\u1ee5 thu\u1ed9c v\u00e0o n\u1ed3ng \u0111\u1ed9 Na\u2082O ho\u1eb7c K\u2082O.<\/li>\r\n<li data-start=\"3291\" data-end=\"3429\"><strong data-start=\"3293\" data-end=\"3311\">L\u01b0u \u00fd b\u1ea3o qu\u1ea3n<\/strong>: \u0110\u01b0\u1ee3c ch\u1ee9a trong <strong data-start=\"3329\" data-end=\"3357\">th\u00f9ng nh\u1ef1a ho\u1eb7c b\u1ed3n inox<\/strong>, tr\u00e1nh d\u00f9ng th\u00f9ng kim lo\u1ea1i th\u01b0\u1eddng do t\u00ednh ki\u1ec1m cao c\u00f3 th\u1ec3 g\u00e2y \u0103n m\u00f2n.<\/li>\r\n<\/ul>\r\n<h3 data-start=\"4533\" data-end=\"4592\"><span class=\"ez-toc-section\" id=\"Natri_Silicat_va_Kali_Silicat_%E2%80%93_Diem_khac_biet\"><\/span><strong data-start=\"4537\" data-end=\"4590\">Natri Silicat v\u00e0 Kali Silicat \u2013 \u0110i\u1ec3m kh\u00e1c bi\u1ec7t<\/strong><span class=\"ez-toc-section-end\"><\/span><\/h3>\r\n<ul data-start=\"4593\" data-end=\"4953\">\r\n<li data-start=\"4593\" data-end=\"4671\"><strong data-start=\"4595\" data-end=\"4622\">Natri Silicat (Na\u2082SiO\u2083)<\/strong> ph\u1ed5 bi\u1ebfn h\u01a1n do <strong data-start=\"4639\" data-end=\"4668\">gi\u00e1 th\u00e0nh r\u1ebb, d\u1ec5 s\u1ea3n xu\u1ea5t<\/strong>.<\/li>\r\n<li data-start=\"4672\" data-end=\"4861\"><strong data-start=\"4674\" data-end=\"4699\">Kali Silicat (K\u2082SiO\u2083)<\/strong> d\u00f9ng trong c\u00e1c \u1ee9ng d\u1ee5ng \u0111\u1eb7c th\u00f9 nh\u01b0:\r\n<ul data-start=\"4745\" data-end=\"4861\">\r\n<li data-start=\"4745\" data-end=\"4782\">Ch\u1ea5t k\u1ebft d\u00ednh ch\u1ecbu nhi\u1ec7t cao.<\/li>\r\n<li data-start=\"4785\" data-end=\"4818\">Ch\u1ed1ng ch\u00e1y trong d\u1ec7t may.<\/li>\r\n<li data-start=\"4821\" data-end=\"4861\">S\u01a1n silicat cho b\u1ec1 m\u1eb7t \u0111\u1eb7c bi\u1ec7t.<\/li>\r\n<\/ul>\r\n<\/li>\r\n<li data-start=\"4862\" data-end=\"4953\">M\u1ed9t s\u1ed1 s\u1ea3n ph\u1ea9m th\u01b0\u01a1ng m\u1ea1i k\u1ebft h\u1ee3p c\u1ea3 hai lo\u1ea1i silicat \u0111\u1ec3 t\u1ed1i \u01b0u t\u00ednh ch\u1ea5t s\u1eed d\u1ee5ng.<\/li>\r\n<\/ul><h2 class=\"wp-block-heading\"><span class=\"ez-toc-section\" id=\"Ung_dung_cua_thuy_tinh_long_trong_cong_nghiep\"><\/span><span style=\"font-weight: 400;\"><strong>\u1ee8ng d\u1ee5ng c\u1ee7a th\u1ee7y tinh l\u1ecfng trong c\u00f4ng nghi\u1ec7p<\/strong><\/span><span class=\"ez-toc-section-end\"><\/span><\/h2><h3 class=\"wp-block-heading\"><span class=\"ez-toc-section\" id=\"Nganh_xay_dung_%E2%80%93_Chong_tham_gia_co_be_tong_tang_do_ben_vat_lieu\"><\/span><span style=\"font-weight: 400;\"><strong>Ng\u00e0nh x\u00e2y d\u1ef1ng &#8211; Ch\u1ed1ng th\u1ea5m, gia c\u1ed1 b\u00ea t\u00f4ng, t\u0103ng \u0111\u1ed9 b\u1ec1n v\u1eadt li\u1ec7u<\/strong><\/span><span class=\"ez-toc-section-end\"><\/span><\/h3><p><span style=\"font-weight: 400;\">Trong ng\u00e0nh x\u00e2y d\u1ef1ng, th\u1ee7y tinh l\u1ecfng \u0111\u01b0\u1ee3c s\u1eed d\u1ee5ng nh\u01b0 m\u1ed9t ch\u1ea5t ch\u1ed1ng th\u1ea5m hi\u1ec7u qu\u1ea3, gi\u00fap gia c\u1ed1 v\u00e0 b\u1ea3o v\u1ec7 c\u00f4ng tr\u00ecnh.<\/span><\/p><ul class=\"wp-block-list\"><li><span style=\"font-weight: 400;\">Ch\u1ed1ng th\u1ea5m cho b\u00ea t\u00f4ng, g\u1ea1ch, v\u1eefa: Gi\u00fap t\u0103ng kh\u1ea3 n\u0103ng ch\u1ed1ng n\u01b0\u1edbc, ng\u0103n ng\u1eeba r\u00eau m\u1ed1c, k\u00e9o d\u00e0i tu\u1ed5i th\u1ecd c\u00f4ng tr\u00ecnh.<\/span><\/li>\r\n\r\n<li><span style=\"font-weight: 400;\">L\u00e0m ph\u1ee5 gia xi m\u0103ng, g\u1ea1ch ch\u1ecbu nhi\u1ec7t: T\u0103ng kh\u1ea3 n\u0103ng ch\u1ecbu l\u1ef1c, h\u1ea1n ch\u1ebf n\u1ee9t v\u1ee1 do co ng\u00f3t nhi\u1ec7t.<\/span><\/li>\r\n\r\n<li><span style=\"font-weight: 400;\">\u1ee8ng d\u1ee5ng trong s\u01a1n ch\u1ed1ng ch\u00e1y, v\u1eefa ch\u1ecbu l\u1eeda: Gi\u00fap t\u01b0\u1eddng, tr\u1ea7n nh\u00e0, v\u1eadt li\u1ec7u x\u00e2y d\u1ef1ng c\u00f3 kh\u1ea3 n\u0103ng ch\u1ecbu nhi\u1ec7t t\u1ed1t h\u01a1n.<\/span><\/li>\r\n\r\n<li><span style=\"font-weight: 400;\">T\u1ea1o l\u1edbp ph\u1ee7 b\u1ea3o v\u1ec7 b\u1ec1 m\u1eb7t: Gi\u00fap ch\u1ed1ng \u0103n m\u00f2n cho c\u00e1c c\u00f4ng tr\u00ecnh ngo\u00e0i tr\u1eddi.<\/span><\/li><\/ul><h3 class=\"wp-block-heading\"><span class=\"ez-toc-section\" id=\"Nganh_xu_ly_nuoc_%E2%80%93_Keo_tu_on_dinh_pH_loai_bo_kim_loai_nang\"><\/span><span style=\"font-weight: 400;\"><strong>Ng\u00e0nh x\u1eed l\u00fd n\u01b0\u1edbc &#8211; Keo t\u1ee5, \u1ed5n \u0111\u1ecbnh pH, lo\u1ea1i b\u1ecf kim lo\u1ea1i n\u1eb7ng<\/strong><\/span><span class=\"ez-toc-section-end\"><\/span><\/h3><p><span style=\"font-weight: 400;\">Th\u1ee7y tinh l\u1ecfng l\u00e0 m\u1ed9t trong nh\u1eefng ch\u1ea5t keo t\u1ee5 hi\u1ec7u qu\u1ea3 trong x\u1eed l\u00fd n\u01b0\u1edbc th\u1ea3i c\u00f4ng nghi\u1ec7p, gi\u00fap gi\u1ea3m chi ph\u00ed x\u1eed l\u00fd n\u01b0\u1edbc v\u00e0 \u0111\u1ea3m b\u1ea3o an to\u00e0n m\u00f4i tr\u01b0\u1eddng.<\/span><\/p><ul class=\"wp-block-list\"><li><span style=\"font-weight: 400;\">Lo\u1ea1i b\u1ecf ion kim lo\u1ea1i n\u1eb7ng (Fe, Mn, Cu, Pb, Zn,&#8230;) gi\u00fap n\u01b0\u1edbc tr\u1edf n\u00ean trong s\u1ea1ch h\u01a1n.<\/span><\/li>\r\n\r\n<li><span style=\"font-weight: 400;\">\u1ed4n \u0111\u1ecbnh \u0111\u1ed9 pH, gi\u1ea3m \u0111\u1ed9 axit trong n\u01b0\u1edbc th\u1ea3i, h\u1ea1n ch\u1ebf \u0103n m\u00f2n \u0111\u01b0\u1eddng \u1ed1ng v\u00e0 thi\u1ebft b\u1ecb.<\/span><\/li>\r\n\r\n<li><span style=\"font-weight: 400;\">H\u1ed7 tr\u1ee3 qu\u00e1 tr\u00ecnh l\u1eafng c\u1eb7n v\u00e0 l\u1ecdc n\u01b0\u1edbc, gi\u00fap lo\u1ea1i b\u1ecf t\u1ea1p ch\u1ea5t hi\u1ec7u qu\u1ea3 h\u01a1n so v\u1edbi ph\u00e8n nh\u00f4m hay PAC.<\/span><\/li>\r\n\r\n<li><span style=\"font-weight: 400;\">S\u1eed d\u1ee5ng trong h\u1ec7 th\u1ed1ng l\u1ecdc n\u01b0\u1edbc RO, h\u1ed3 b\u01a1i, s\u1ea3n xu\u1ea5t n\u01b0\u1edbc u\u1ed1ng c\u00f4ng nghi\u1ec7p.<\/span><\/li><\/ul>\r\n<blockquote>\r\n<p><span style=\"text-decoration: underline;\"><strong>\ub354 \ubcf4\uae30:<\/strong><\/span> <a href=\"https:\/\/hoachatlocthien.com\/ko\/hoa-chat-xu-ly-nuoc\/\">N\u01a1i b\u00e1n h\u00f3a ch\u1ea5t x\u1eed l\u00fd n\u01b0\u1edbc<\/a><\/p>\r\n<\/blockquote>\r\n<p><img decoding=\"async\" class=\"aligncenter wp-image-657 lazyload\" data-src=\"https:\/\/hoachatlocthien.com\/wp-content\/uploads\/2023\/10\/xu-ly-nuoc-thai-cong-nghiep.webp\" alt=\"\" width=\"600\" height=\"400\" data-srcset=\"https:\/\/hoachatlocthien.com\/wp-content\/uploads\/2023\/10\/xu-ly-nuoc-thai-cong-nghiep.webp 800w, https:\/\/hoachatlocthien.com\/wp-content\/uploads\/2023\/10\/xu-ly-nuoc-thai-cong-nghiep-500x333.webp 500w\" data-sizes=\"(max-width: 600px) 100vw, 600px\" src=\"data:image\/gif;base64,R0lGODlhAQABAAAAACH5BAEKAAEALAAAAAABAAEAAAICTAEAOw==\" style=\"--smush-placeholder-width: 600px; --smush-placeholder-aspect-ratio: 600\/400;\" \/><\/p><h3 class=\"wp-block-heading\"><span class=\"ez-toc-section\" id=\"Nganh_det_nhuom_%E2%80%93_On_dinh_mau_vai_chong_chay\"><\/span><span style=\"font-weight: 400;\"><strong>Ng\u00e0nh d\u1ec7t nhu\u1ed9m &#8211; \u1ed4n \u0111\u1ecbnh m\u00e0u v\u1ea3i, ch\u1ed1ng ch\u00e1y<\/strong><\/span><span class=\"ez-toc-section-end\"><\/span><\/h3><p><span style=\"font-weight: 400;\">Trong ng\u00e0nh d\u1ec7t nhu\u1ed9m, th\u1ee7y tinh l\u1ecfng \u0111\u01b0\u1ee3c d\u00f9ng l\u00e0m ch\u1ea5t \u1ed5n \u0111\u1ecbnh trong nhu\u1ed9m m\u00e0u, gi\u00fap m\u00e0u s\u1eafc b\u1ec1n l\u00e2u, kh\u00f4ng phai khi gi\u1eb7t.<\/span><\/p><ul class=\"wp-block-list\"><li><span style=\"font-weight: 400;\">T\u0103ng \u0111\u1ed9 b\u1ec1n m\u00e0u, gi\u1ea3m hi\u1ec7n t\u01b0\u1ee3ng loang m\u00e0u, gi\u00fap s\u1ee3i v\u1ea3i b\u1ec1n h\u01a1n.<\/span><\/li>\r\n\r\n<li><span style=\"font-weight: 400;\">\u1ee8ng d\u1ee5ng trong qu\u1ea7n \u00e1o b\u1ea3o h\u1ed9, r\u00e8m c\u1eeda ch\u1ed1ng ch\u00e1y, gi\u00fap s\u1ea3n ph\u1ea9m \u0111\u1ea1t ti\u00eau chu\u1ea9n an to\u00e0n ch\u00e1y n\u1ed5.<\/span><\/li>\r\n\r\n<li><span style=\"font-weight: 400;\">Gi\u00fap v\u1ea3i m\u1ec1m h\u01a1n, gi\u1ea3m t\u0129nh \u0111i\u1ec7n, h\u1ea1n ch\u1ebf x\u01a1 v\u1ea3i trong qu\u00e1 tr\u00ecnh s\u1eed d\u1ee5ng.<\/span><\/li><\/ul><h3 class=\"wp-block-heading\"><span class=\"ez-toc-section\" id=\"Nganh_san_xuat_giay_%E2%80%93_Gia_co_be_mat_tang_do_ben_va_chong_am\"><\/span><span style=\"font-weight: 400;\"><strong>Ng\u00e0nh s\u1ea3n xu\u1ea5t gi\u1ea5y &#8211; Gia c\u1ed1 b\u1ec1 m\u1eb7t, t\u0103ng \u0111\u1ed9 b\u1ec1n v\u00e0 ch\u1ed1ng \u1ea9m<\/strong><\/span><span class=\"ez-toc-section-end\"><\/span><\/h3><p><span style=\"font-weight: 400;\">Th\u1ee7y tinh l\u1ecfng \u0111\u00f3ng vai tr\u00f2 quan tr\u1ecdng trong s\u1ea3n xu\u1ea5t gi\u1ea5y, \u0111\u1eb7c bi\u1ec7t l\u00e0 bao b\u00ec carton, gi\u1ea5y kraft, gi\u1ea5y ch\u1ed1ng th\u1ea5m n\u01b0\u1edbc.<\/span><\/p><ul class=\"wp-block-list\"><li><span style=\"font-weight: 400;\">T\u0103ng \u0111\u1ed9 b\u1ec1n c\u01a1 h\u1ecdc cho gi\u1ea5y, gi\u00fap s\u1ea3n ph\u1ea9m ch\u1ecbu l\u1ef1c t\u1ed1t h\u01a1n, h\u1ea1n ch\u1ebf r\u00e1ch, g\u00e3y.<\/span><\/li>\r\n\r\n<li><span style=\"font-weight: 400;\">Ch\u1ed1ng \u1ea9m, ch\u1ed1ng th\u1ea5m n\u01b0\u1edbc, gi\u00fap b\u1ea3o v\u1ec7 h\u00e0ng h\u00f3a b\u00ean trong bao b\u00ec khi v\u1eadn chuy\u1ec3n.<\/span><\/li>\r\n\r\n<li><span style=\"font-weight: 400;\">L\u00e0m ch\u1ea5t li\u00ean k\u1ebft trong s\u1ea3n xu\u1ea5t gi\u1ea5y kraft, t\u1ea1o b\u1ec1 m\u1eb7t l\u00e1ng m\u1ecbn, t\u0103ng \u0111\u1ed9 b\u1ec1n g\u1ea5p n\u1ebfp.<\/span><\/li><\/ul><h3 class=\"wp-block-heading\"><span class=\"ez-toc-section\" id=\"Nganh_san_xuat_keo_dan_cong_nghiep_%E2%80%93_Chat_ket_dinh_ben_vung\"><\/span><span style=\"font-weight: 400;\"><strong>Ng\u00e0nh s\u1ea3n xu\u1ea5t keo d\u00e1n c\u00f4ng nghi\u1ec7p &#8211; Ch\u1ea5t k\u1ebft d\u00ednh b\u1ec1n v\u1eefng<\/strong><\/span><span class=\"ez-toc-section-end\"><\/span><\/h3><p><span style=\"font-weight: 400;\">Th\u1ee7y tinh l\u1ecfng l\u00e0 nguy\u00ean li\u1ec7u ch\u00ednh trong s\u1ea3n xu\u1ea5t keo silicat, gi\u00fap t\u1ea1o ra c\u00e1c s\u1ea3n ph\u1ea9m k\u1ebft d\u00ednh m\u1ea1nh, ch\u1ecbu nhi\u1ec7t t\u1ed1t.<\/span><\/p><ul class=\"wp-block-list\"><li><span style=\"font-weight: 400;\">\u1ee8ng d\u1ee5ng trong keo d\u00e1n g\u1ed7, keo d\u00e1n gi\u1ea5y, keo d\u00e1n g\u1ed1m s\u1ee9.<\/span><\/li>\r\n\r\n<li><span style=\"font-weight: 400;\">L\u00e0m ch\u1ea5t li\u00ean k\u1ebft trong s\u1ea3n xu\u1ea5t t\u1ea5m c\u00e1ch nhi\u1ec7t, g\u1ea1ch ch\u1ecbu l\u1eeda.<\/span><\/li>\r\n\r\n<li><span style=\"font-weight: 400;\">Keo d\u00e1n an to\u00e0n, kh\u00f4ng \u0111\u1ed9c h\u1ea1i, kh\u00f4ng g\u00e2y \u00f4 nhi\u1ec5m m\u00f4i tr\u01b0\u1eddng.<\/span><\/li><\/ul><h2 class=\"wp-block-heading\"><span class=\"ez-toc-section\" id=\"Huong_dan_bao_quan_Luu_y_khi_su_dung\"><\/span><span style=\"font-weight: 400;\"><strong>H\u01b0\u1edbng d\u1eabn b\u1ea3o qu\u1ea3n &amp; L\u01b0u \u00fd khi s\u1eed d\u1ee5ng<\/strong><\/span><span class=\"ez-toc-section-end\"><\/span><\/h2><h3 class=\"wp-block-heading\"><span class=\"ez-toc-section\" id=\"Cach_bao_quan\"><\/span><span style=\"font-weight: 400;\"><strong>C\u00e1ch b\u1ea3o qu\u1ea3n<\/strong><\/span><span class=\"ez-toc-section-end\"><\/span><\/h3><ul class=\"wp-block-list\"><li><span style=\"font-weight: 400;\">L\u01b0u tr\u1eef trong th\u00f9ng nh\u1ef1a ho\u1eb7c th\u00f9ng kim lo\u1ea1i kh\u00f4ng g\u1ec9.<\/span><\/li>\r\n\r\n<li><span style=\"font-weight: 400;\">Tr\u00e1nh ti\u1ebfp x\u00fac v\u1edbi kh\u00f4ng kh\u00ed qu\u00e1 l\u00e2u \u0111\u1ec3 tr\u00e1nh \u0111\u00f4ng c\u1ee9ng.<\/span><\/li>\r\n\r\n<li><span style=\"font-weight: 400;\">Kh\u00f4ng \u0111\u1ec3 g\u1ea7n axit m\u1ea1nh, tr\u00e1nh ph\u1ea3n \u1ee9ng h\u00f3a h\u1ecdc kh\u00f4ng mong mu\u1ed1n.<\/span><\/li><\/ul><h3 class=\"wp-block-heading\"><span class=\"ez-toc-section\" id=\"Luu_y_an_toan\"><\/span><span style=\"font-weight: 400;\"><strong>L\u01b0u \u00fd an to\u00e0n<\/strong><\/span><span class=\"ez-toc-section-end\"><\/span><\/h3><ul class=\"wp-block-list\"><li><span style=\"font-weight: 400;\">Mang g\u0103ng tay, k\u00ednh b\u1ea3o h\u1ed9 khi ti\u1ebfp x\u00fac v\u1edbi th\u1ee7y tinh l\u1ecfng.<\/span><\/li>\r\n\r\n<li><span style=\"font-weight: 400;\">Tr\u00e1nh ti\u1ebfp x\u00fac tr\u1ef1c ti\u1ebfp v\u1edbi da v\u00e0 m\u1eaft, n\u1ebfu d\u00ednh ph\u1ea3i r\u1eeda ngay v\u1edbi n\u01b0\u1edbc s\u1ea1ch.<\/span><\/li><\/ul><h2 class=\"wp-block-heading\"><span class=\"ez-toc-section\" id=\"Lien_he_dat_hang_thuy_tinh_long_tai_Loc_Thien\"><\/span><span style=\"font-weight: 400;\"><strong>Li\u00ean h\u1ec7 \u0111\u1eb7t h\u00e0ng th\u1ee7y tinh l\u1ecfng t\u1ea1i L\u1ed9c Thi\u00ean<\/strong><\/span><span class=\"ez-toc-section-end\"><\/span><\/h2><p><span style=\"font-weight: 400;\">Khi ch\u1ecdn <a href=\"https:\/\/hoachatlocthien.com\/ko\/natri-silicat-na2sio3-thuy-tinh-long\/\">mua th\u1ee7y tinh l\u1ecfng<\/a> t\u1ea1i H\u00f3a Ch\u1ea5t L\u1ed9c Thi\u00ean, doanh nghi\u1ec7p nh\u1eadn \u0111\u01b0\u1ee3c:<\/span><\/p><ul class=\"wp-block-list\"><li><span style=\"font-weight: 400;\"><strong>Ch\u1ea5t l\u01b0\u1ee3ng \u0111\u1ea1t chu\u1ea9n:<\/strong> \u0110\u1ea7y \u0111\u1ee7 ch\u1ee9ng nh\u1eadn MSDS, COA, ISO 9001:2015.<\/span><\/li>\r\n\r\n<li><span style=\"font-weight: 400;\"><strong>Ngu\u1ed3n h\u00e0ng d\u1ed3i d\u00e0o:<\/strong> H\u1ec7 th\u1ed1ng 6 kho b\u00e3i to\u00e0n qu\u1ed1c, s\u1eb5n h\u00e0ng s\u1ed1 l\u01b0\u1ee3ng l\u1edbn.<\/span><\/li>\r\n\r\n<li><span style=\"font-weight: 400;\"><strong>\uacbd\uc7c1\ub825 \uc788\ub294 \uac00\uaca9:<\/strong> Nh\u1eadp kh\u1ea9u tr\u1ef1c ti\u1ebfp, gi\u1ea3m chi ph\u00ed trung gian, \u01b0u \u0111\u00e3i l\u1edbn cho \u0111\u01a1n h\u00e0ng s\u1ed1 l\u01b0\u1ee3ng l\u1edbn.<\/span><\/li>\r\n\r\n<li><span style=\"font-weight: 400;\">H\u1ed7 tr\u1ee3 k\u1ef9 thu\u1eadt chuy\u00ean s\u00e2u: \u0110\u1ed9i ng\u0169 chuy\u00ean gia h\u00f3a ch\u1ea5t t\u01b0 v\u1ea5n t\u1eadn t\u00ecnh.<\/span><ul class=\"wp-block-list\"><li><span style=\"font-weight: 400;\"><strong>\uc0c1\ub2f4 \uc804\ud654:<\/strong> <a href=\"tel:0979891929\">0979 89 19 29<\/a><\/span><\/li>\r\n\r\n<li><span style=\"font-weight: 400;\"><strong>Website<\/strong><\/span><strong>: <\/strong><a href=\"https:\/\/hoachatlocthien.com\/ko\/\"><span style=\"font-weight: 400;\">hoachatlocthien.com<\/span><\/a><\/li>\r\n\r\n<\/ul><\/li><\/ul><figure class=\"wp-block-image size-full\"><img decoding=\"async\" width=\"1000\" height=\"730\" data-sizes=\"(max-width: 1000px) 100vw, 1000px\" class=\"wp-image-1405 lazyload\" data-src=\"https:\/\/hoachatlocthien.com\/wp-content\/uploads\/2023\/12\/XE.png\" alt=\"hoachatlocthien\" data-srcset=\"https:\/\/hoachatlocthien.com\/wp-content\/uploads\/2023\/12\/XE.png 1000w, https:\/\/hoachatlocthien.com\/wp-content\/uploads\/2023\/12\/XE-500x365.png 500w\" src=\"data:image\/gif;base64,R0lGODlhAQABAAAAACH5BAEKAAEALAAAAAABAAEAAAICTAEAOw==\" style=\"--smush-placeholder-width: 1000px; --smush-placeholder-aspect-ratio: 1000\/730;\" \/><\/figure><p class=\"has-text-align-center\"><i><span style=\"font-weight: 400;\">Giao h\u00e0ng t\u1eadn n\u01a1i &#8211; H\u1ed7 tr\u1ee3 k\u1ef9 thu\u1eadt &#8211; Cam k\u1ebft ch\u1ea5t l\u01b0\u1ee3ng!<\/span><\/i><span style=\"font-weight: 400;\">\u00a0<\/span><\/p><div id=\"rank-math-faq\" class=\"rank-math-block\">\n<div class=\"rank-math-list\">\n<div id=\"faq-question-1740725019633\" class=\"rank-math-list-item\">\n<h3 class=\"rank-math-question\"><span class=\"ez-toc-section\" id=\"Thuy_tinh_long_co_an_toan_cho_con_nguoi_khong\"><\/span><span style=\"font-weight: 400\"><strong>Th\u1ee7y tinh l\u1ecfng c\u00f3 an to\u00e0n cho con ng\u01b0\u1eddi kh\u00f4ng?<\/strong><\/span><span class=\"ez-toc-section-end\"><\/span><\/h3>\n<div class=\"rank-math-answer\">\n\n<p><span style=\"font-weight: 400\">Th\u1ee7y tinh l\u1ecfng c\u00f3 t\u00ednh ki\u1ec1m m\u1ea1nh (pH 11-12) v\u00e0 c\u00f3 th\u1ec3 g\u00e2y k\u00edch \u1ee9ng da, m\u1eaft ho\u1eb7c \u0111\u01b0\u1eddng h\u00f4 h\u1ea5p n\u1ebfu ti\u1ebfp x\u00fac tr\u1ef1c ti\u1ebfp. Khi s\u1eed d\u1ee5ng, c\u1ea7n \u0111eo g\u0103ng tay b\u1ea3o h\u1ed9, k\u00ednh b\u1ea3o v\u1ec7 m\u1eaft v\u00e0 tr\u00e1nh h\u00edt ph\u1ea3i h\u01a1i dung d\u1ecbch. <\/span><br \/><span style=\"font-weight: 400\">N\u1ebfu b\u1ecb d\u00ednh l\u00ean da, r\u1eeda ngay b\u1eb1ng n\u01b0\u1edbc s\u1ea1ch trong \u00edt nh\u1ea5t 15 ph\u00fat. Trong c\u00f4ng nghi\u1ec7p th\u1ef1c ph\u1ea9m, th\u1ee7y tinh l\u1ecfng \u0111\u00f4i khi \u0111\u01b0\u1ee3c s\u1eed d\u1ee5ng nh\u01b0ng ph\u1ea3i qua quy tr\u00ecnh x\u1eed l\u00fd \u0111\u1eb7c bi\u1ec7t \u0111\u1ec3 \u0111\u1ea3m b\u1ea3o an to\u00e0n.<\/span><\/p>\n\n<\/div>\n<\/div>\n<div id=\"faq-question-1740725031209\" class=\"rank-math-list-item\">\n<h3 class=\"rank-math-question\"><span class=\"ez-toc-section\" id=\"Thuy_tinh_long_co_the_su_dung_trong_san_xuat_gom_su_khong\"><\/span><span style=\"font-weight: 400\"><strong>Th\u1ee7y tinh l\u1ecfng c\u00f3 th\u1ec3 s\u1eed d\u1ee5ng trong s\u1ea3n xu\u1ea5t g\u1ed1m s\u1ee9 kh\u00f4ng?<\/strong><\/span><span class=\"ez-toc-section-end\"><\/span><\/h3>\n<div class=\"rank-math-answer\">\n\n<p><span style=\"font-weight: 400\">C\u00f3. Trong ng\u00e0nh g\u1ed1m s\u1ee9, th\u1ee7y tinh l\u1ecfng \u0111\u01b0\u1ee3c d\u00f9ng l\u00e0m ch\u1ea5t k\u1ebft d\u00ednh trong men g\u1ed1m, gi\u00fap t\u0103ng c\u01b0\u1eddng \u0111\u1ed9 b\u1ec1n, kh\u1ea3 n\u0103ng ch\u1ecbu nhi\u1ec7t v\u00e0 \u0111\u1ed9 b\u00e1m d\u00ednh c\u1ee7a l\u1edbp men l\u00ean b\u1ec1 m\u1eb7t g\u1ed1m. Ngo\u00e0i ra, n\u00f3 c\u00f2n \u0111\u01b0\u1ee3c s\u1eed d\u1ee5ng nh\u01b0 m\u1ed9t lo\u1ea1i keo ch\u1ecbu nhi\u1ec7t \u0111\u1ec3 gia c\u1ed1 c\u00e1c v\u1eadt li\u1ec7u ch\u1ecbu l\u1eeda, \u0111\u1eb7c bi\u1ec7t l\u00e0 trong s\u1ea3n xu\u1ea5t g\u1ea1ch ch\u1ecbu l\u1eeda v\u00e0 g\u1ed1m k\u1ef9 thu\u1eadt cao.<\/span><\/p>\n\n<\/div>\n<\/div>\n<div id=\"faq-question-1740725037761\" class=\"rank-math-list-item\">\n<h3 class=\"rank-math-question\"><span class=\"ez-toc-section\" id=\"Thuy_tinh_long_co_the_tai_su_dung_khong\"><\/span><span style=\"font-weight: 400\"><strong>Th\u1ee7y tinh l\u1ecfng c\u00f3 th\u1ec3 t\u00e1i s\u1eed d\u1ee5ng kh\u00f4ng?<\/strong><\/span><span class=\"ez-toc-section-end\"><\/span><\/h3>\n<div class=\"rank-math-answer\">\n\n<p><span style=\"font-weight: 400\">Th\u1ee7y tinh l\u1ecfng kh\u00f4ng th\u1ec3 t\u00e1i s\u1eed d\u1ee5ng tr\u1ef1c ti\u1ebfp n\u1ebfu \u0111\u00e3 pha lo\u00e3ng ho\u1eb7c \u0111\u00e3 ph\u1ea3n \u1ee9ng v\u1edbi c\u00e1c v\u1eadt li\u1ec7u kh\u00e1c. Tuy nhi\u00ean, trong m\u1ed9t s\u1ed1 \u1ee9ng d\u1ee5ng c\u00f4ng nghi\u1ec7p nh\u01b0 x\u1eed l\u00fd n\u01b0\u1edbc ho\u1eb7c s\u1ea3n xu\u1ea5t keo silicat, dung d\u1ecbch c\u00f3 th\u1ec3 \u0111\u01b0\u1ee3c l\u1ecdc v\u00e0 t\u00e1i ch\u1ebf m\u1ed9t ph\u1ea7n \u0111\u1ec3 gi\u1ea3m thi\u1ec3u chi ph\u00ed nguy\u00ean li\u1ec7u. N\u1ebfu kh\u00f4ng th\u1ec3 t\u00e1i s\u1eed d\u1ee5ng, c\u1ea7n x\u1eed l\u00fd \u0111\u00fang c\u00e1ch \u0111\u1ec3 tr\u00e1nh g\u00e2y \u00f4 nhi\u1ec5m m\u00f4i tr\u01b0\u1eddng.<\/span><\/p>\n\n<\/div>\n<\/div>\n<div id=\"faq-question-1740725048095\" class=\"rank-math-list-item\">\n<h3 class=\"rank-math-question\"><span class=\"ez-toc-section\" id=\"Thuy_tinh_long_co_bi_dong_cung_khong_Cach_khac_phuc_khi_bi_dong_dac\"><\/span><span style=\"font-weight: 400\"><strong>Th\u1ee7y tinh l\u1ecfng c\u00f3 b\u1ecb \u0111\u00f4ng c\u1ee9ng kh\u00f4ng? C\u00e1ch kh\u1eafc ph\u1ee5c khi b\u1ecb \u0111\u00f4ng \u0111\u1eb7c?<\/strong><\/span><span class=\"ez-toc-section-end\"><\/span><\/h3>\n<div class=\"rank-math-answer\">\n\n<p>trong b\u1ec3 n\u01b0\u1edbc \u1ea5m (~40-50\u00b0C) \u0111\u1ec3 l\u00e0m lo\u00e3ng k\u1ebft tinh.<br \/>Khu\u1ea5y \u0111\u1ec1u v\u00e0 th\u00eam n\u01b0\u1edbc (theo t\u1ef7 l\u1ec7 ph\u00f9 h\u1ee3p) \u0111\u1ec3 ph\u1ee5c h\u1ed3i \u0111\u1ed9 nh\u1edbt ban \u0111\u1ea7u.<br \/>Tr\u00e1nh \u0111\u1ec3 th\u1ee7y tinh l\u1ecfng ti\u1ebfp x\u00fac v\u1edbi kh\u00f4ng kh\u00ed qu\u00e1 l\u00e2u \u0111\u1ec3 h\u1ea1n ch\u1ebf qu\u00e1 tr\u00ecnh kh\u00f4 c\u1ee9ng.<\/p>\n\n<\/div>\n<\/div>\n<div id=\"faq-question-1740725076017\" class=\"rank-math-list-item\">\n<h3 class=\"rank-math-question\"><span class=\"ez-toc-section\" id=\"Thuy_tinh_long_co_bi_dong_cung_khong_Cach_khac_phuc_khi_bi_dong_dac-2\"><\/span>Th\u1ee7y tinh l\u1ecfng c\u00f3 b\u1ecb \u0111\u00f4ng c\u1ee9ng kh\u00f4ng? C\u00e1ch kh\u1eafc ph\u1ee5c khi b\u1ecb \u0111\u00f4ng \u0111\u1eb7c?<span class=\"ez-toc-section-end\"><\/span><\/h3>\n<div class=\"rank-math-answer\">\n\n<p>C\u00f3. N\u1ebfu b\u1ea3o qu\u1ea3n kh\u00f4ng \u0111\u00fang c\u00e1ch, th\u1ee7y tinh l\u1ecfng c\u00f3 th\u1ec3 b\u1ecb \u0111\u00f4ng \u0111\u1eb7c ho\u1eb7c k\u1ebft tinh khi ti\u1ebfp x\u00fac l\u00e2u v\u1edbi kh\u00f4ng kh\u00ed ho\u1eb7c khi nhi\u1ec7t \u0111\u1ed9 xu\u1ed1ng qu\u00e1 th\u1ea5p. \u0110\u1ec3 kh\u1eafc ph\u1ee5c, c\u00f3 th\u1ec3:<br \/> + H\u00e2m n\u00f3ng nh\u1eb9 dung d\u1ecbch b\u1eb1ng c\u00e1ch \u0111\u1eb7t trong b\u1ec3 n\u01b0\u1edbc \u1ea5m (~40-50\u00b0C) \u0111\u1ec3 l\u00e0m lo\u00e3ng k\u1ebft tinh.<br \/> + Khu\u1ea5y \u0111\u1ec1u v\u00e0 th\u00eam n\u01b0\u1edbc (theo t\u1ef7 l\u1ec7 ph\u00f9 h\u1ee3p) \u0111\u1ec3 ph\u1ee5c h\u1ed3i \u0111\u1ed9 nh\u1edbt ban \u0111\u1ea7u.<br \/> + Tr\u00e1nh \u0111\u1ec3 th\u1ee7y tinh l\u1ecfng ti\u1ebfp x\u00fac v\u1edbi kh\u00f4ng kh\u00ed qu\u00e1 l\u00e2u \u0111\u1ec3 h\u1ea1n ch\u1ebf qu\u00e1 tr\u00ecnh kh\u00f4 c\u1ee9ng.<\/p>\n\n<\/div>\n<\/div>\n<div id=\"faq-question-1740725111793\" class=\"rank-math-list-item\">\n<h3 class=\"rank-math-question\"><span class=\"ez-toc-section\" id=\"Thuy_tinh_long_co_anh_huong_den_moi_truong_khong\"><\/span><span style=\"font-weight: 400\"><strong>Th\u1ee7y tinh l\u1ecfng c\u00f3 \u1ea3nh h\u01b0\u1edfng \u0111\u1ebfn m\u00f4i tr\u01b0\u1eddng kh\u00f4ng?<\/strong><\/span><span class=\"ez-toc-section-end\"><\/span><\/h3>\n<div class=\"rank-math-answer\">\n\n<p><span style=\"font-weight: 400\">Th\u1ee7y tinh l\u1ecfng kh\u00f4ng \u0111\u1ed9c h\u1ea1i nh\u01b0ng c\u00f3 t\u00ednh ki\u1ec1m cao, n\u1ebfu th\u1ea3i ra m\u00f4i tr\u01b0\u1eddng m\u00e0 kh\u00f4ng qua x\u1eed l\u00fd c\u00f3 th\u1ec3 \u1ea3nh h\u01b0\u1edfng \u0111\u1ebfn h\u1ec7 sinh th\u00e1i n\u01b0\u1edbc, l\u00e0m thay \u0111\u1ed5i \u0111\u1ed9 pH c\u1ee7a ngu\u1ed3n n\u01b0\u1edbc t\u1ef1 nhi\u00ean. \u0110\u1ec3 gi\u1ea3m t\u00e1c \u0111\u1ed9ng m\u00f4i tr\u01b0\u1eddng:<br \/>+ Pha lo\u00e3ng v\u00e0 trung h\u00f2a dung d\u1ecbch tr\u01b0\u1edbc khi th\u1ea3i b\u1ecf.<br \/>+ S\u1eed d\u1ee5ng h\u1ec7 th\u1ed1ng x\u1eed l\u00fd n\u01b0\u1edbc th\u1ea3i c\u00f4ng nghi\u1ec7p \u0111\u1ec3 lo\u1ea1i b\u1ecf c\u00e1c ion kim lo\u1ea1i n\u1eb7ng c\u00f2n s\u00f3t l\u1ea1i.<br \/>+ Tu\u00e2n th\u1ee7 c\u00e1c quy \u0111\u1ecbnh v\u1ec1 x\u1eed l\u00fd h\u00f3a ch\u1ea5t \u0111\u1ec3 tr\u00e1nh g\u00e2y \u00f4 nhi\u1ec5m m\u00f4i tr\u01b0\u1eddng.<\/span><\/p>\n\n<\/div>\n<\/div>\n<\/div>\n<\/div>","protected":false},"excerpt":{"rendered":"<p>Trong nhi\u1ec1u ng\u00e0nh c\u00f4ng nghi\u1ec7p, t\u1eeb x\u00e2y d\u1ef1ng, x\u1eed l\u00fd n\u01b0\u1edbc, \u0111\u1ebfn s\u1ea3n xu\u1ea5t gi\u1ea5y, d\u1ec7t nhu\u1ed9m v\u00e0 keo d\u00e1n, th\u1ee7y tinh l\u1ecfng (Natri Silicat &#8211; Na\u2082SiO\u2083) \u0111\u00f3ng vai tr\u00f2 quan tr\u1ecdng nh\u1edd v\u00e0o kh\u1ea3 n\u0103ng k\u1ebft d\u00ednh m\u1ea1nh, ch\u1ed1ng th\u1ea5m hi\u1ec7u qu\u1ea3 v\u00e0 ch\u1ecbu nhi\u1ec7t t\u1ed1t. Kh\u00f4ng ch\u1ec9 gi\u00fap gia c\u1ed1 v\u1eadt li\u1ec7u v\u00e0 [&#8230;]\n","protected":false},"author":1,"featured_media":5639,"comment_status":"closed","ping_status":"open","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"footnotes":""},"categories":[16],"tags":[],"class_list":["post-5620","post","type-post","status-publish","format-standard","has-post-thumbnail","hentry","category-tin-tuc"],"acf":[],"_links":{"self":[{"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/posts\/5620","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/users\/1"}],"replies":[{"embeddable":true,"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/comments?post=5620"}],"version-history":[{"count":17,"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/posts\/5620\/revisions"}],"predecessor-version":[{"id":5665,"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/posts\/5620\/revisions\/5665"}],"wp:featuredmedia":[{"embeddable":true,"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/media\/5639"}],"wp:attachment":[{"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/media?parent=5620"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/categories?post=5620"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/tags?post=5620"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}