{"id":9044,"date":"2026-05-06T08:00:00","date_gmt":"2026-05-06T08:00:00","guid":{"rendered":"https:\/\/hoachatlocthien.com\/noi-ban-naocl-10-12-tai-binh-duong\/"},"modified":"2026-05-20T10:11:03","modified_gmt":"2026-05-20T03:11:03","slug":"noi-ban-naocl-10-12-tai-binh-duong-2","status":"publish","type":"post","link":"https:\/\/hoachatlocthien.com\/ko\/noi-ban-naocl-10-12-tai-binh-duong-2","title":{"rendered":"N\u01a1i B\u00e1n NaOCl 10\u201312% (Javen C\u00f4ng Nghi\u1ec7p) T\u1ea1i B\u00ecnh D\u01b0\u01a1ng"},"content":{"rendered":"<article>\n<header class=\"hero\">\n<div class=\"kicker\">Javen 10-12% B\u00ecnh D\u01b0\u01a1ng<\/div>\n<h1>N\u01a1i B\u00e1n NaOCl 10\u201312% (Javen C\u00f4ng Nghi\u1ec7p) T\u1ea1i B\u00ecnh D\u01b0\u01a1ng<\/h1>\n<p class=\"meta\">Bien soan boi doi ngu ky thuat <strong>Hoa Chat Loc Thien<\/strong>.<\/p>\n<p><strong>NaOCl 10\u201312% (Javen c\u00f4ng nghi\u1ec7p)<\/strong> \u0111\u01b0\u1ee3c d\u00f9ng r\u1ed9ng r\u00e3i t\u1ea1i c\u00e1c nh\u00e0 m\u00e1y B\u00ecnh D\u01b0\u01a1ng \u0111\u1ec3 kh\u1eed tr\u00f9ng n\u01b0\u1edbc, t\u1ea9y tr\u1eafng v\u1ea3i, x\u1eed l\u00fd n\u01b0\u1edbc th\u1ea3i. L\u1ed9c Thi\u00ean l\u00e0 m\u1ed9t trong nh\u1eefng \u0111\u01a1n v\u1ecb cung c\u1ea5p Javen c\u00f4ng nghi\u1ec7p t\u01b0\u01a1i t\u1ea1i B\u00ecnh D\u01b0\u01a1ng.<\/p>\n<p class=\"note\">Noi dung tham khao, vui long doi chieu MSDS.<\/p>\n<\/header>\n<figure><img decoding=\"async\" class=\"thumb lazyload\" data-src=\"https:\/\/hoachatlocthien.com\/wp-content\/uploads\/2023\/12\/Javen.webp\" alt=\"Ho\u00e1 ch\u1ea5t Javen 10% -12 % m\u00e0u v\u00e0ng nh\u1ea1t\" width=\"900\" height=\"500\" src=\"data:image\/gif;base64,R0lGODlhAQABAAAAACH5BAEKAAEALAAAAAABAAEAAAICTAEAOw==\" style=\"--smush-placeholder-width: 900px; --smush-placeholder-aspect-ratio: 900\/500;\"><figcaption class=\"meta\" style=\"text-align:center\">Ho\u00e1 ch\u1ea5t Javen 10% -12 % m\u00e0u v\u00e0ng nh\u1ea1t<\/figcaption><\/figure>\n<div class=\"tag-list\"><span>NaOCl 10-12%<\/span><span>Javen B\u00ecnh D\u01b0\u01a1ng<\/span><span>Javen c\u00f4ng nghi\u1ec7p<\/span><span>NaOCl B\u00ecnh D\u01b0\u01a1ng<\/span><span>Javen 12%<\/span><\/div>\n<section id=\"tieu-chuan\">\n<div id=\"ez-toc-container\" class=\"ez-toc-v2_0_72 counter-hierarchy ez-toc-counter ez-toc-grey ez-toc-container-direction\">\n<div class=\"ez-toc-title-container\">\n<p class=\"ez-toc-title\" style=\"cursor:inherit\">N\u1ed9i dung<\/p>\n<span class=\"ez-toc-title-toggle\"><a href=\"#\" class=\"ez-toc-pull-right ez-toc-btn ez-toc-btn-xs ez-toc-btn-default ez-toc-toggle\" aria-label=\"Toggle Table of Content\"><span class=\"ez-toc-js-icon-con\"><span class=\"\"><span class=\"eztoc-hide\" style=\"display:none;\">Toggle<\/span><span class=\"ez-toc-icon-toggle-span\"><svg style=\"fill: #dd3333;color:#dd3333\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\" class=\"list-377408\" width=\"20px\" height=\"20px\" viewBox=\"0 0 24 24\" fill=\"none\"><path d=\"M6 6H4v2h2V6zm14 0H8v2h12V6zM4 11h2v2H4v-2zm16 0H8v2h12v-2zM4 16h2v2H4v-2zm16 0H8v2h12v-2z\" fill=\"currentColor\"><\/path><\/svg><svg style=\"fill: #dd3333;color:#dd3333\" class=\"arrow-unsorted-368013\" xmlns=\"http:\/\/www.w3.org\/2000\/svg\" width=\"10px\" height=\"10px\" viewBox=\"0 0 24 24\" version=\"1.2\" baseProfile=\"tiny\"><path d=\"M18.2 9.3l-6.2-6.3-6.2 6.3c-.2.2-.3.4-.3.7s.1.5.3.7c.2.2.4.3.7.3h11c.3 0 .5-.1.7-.3.2-.2.3-.5.3-.7s-.1-.5-.3-.7zM5.8 14.7l6.2 6.3 6.2-6.3c.2-.2.3-.5.3-.7s-.1-.5-.3-.7c-.2-.2-.4-.3-.7-.3h-11c-.3 0-.5.1-.7.3-.2.2-.3.5-.3.7s.1.5.3.7z\"\/><\/svg><\/span><\/span><\/span><\/a><\/span><\/div>\n<nav><ul class='ez-toc-list ez-toc-list-level-1 ' ><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-1\" href=\"https:\/\/hoachatlocthien.com\/ko\/noi-ban-naocl-10-12-tai-binh-duong-2\/#1_Tieu_chuan_NaOCl_10%E2%80%9312_cong_nghiep\" title=\"1. Ti\u00eau chu\u1ea9n NaOCl 10\u201312% c\u00f4ng nghi\u1ec7p\">1. Ti\u00eau chu\u1ea9n NaOCl 10\u201312% c\u00f4ng nghi\u1ec7p<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-2\" href=\"https:\/\/hoachatlocthien.com\/ko\/noi-ban-naocl-10-12-tai-binh-duong-2\/#2_Ung_dung_NaOCl_10%E2%80%9312_tai_Binh_Duong\" title=\"2. \u1ee8ng d\u1ee5ng NaOCl 10\u201312% t\u1ea1i B\u00ecnh D\u01b0\u01a1ng\">2. \u1ee8ng d\u1ee5ng NaOCl 10\u201312% t\u1ea1i B\u00ecnh D\u01b0\u01a1ng<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-3\" href=\"https:\/\/hoachatlocthien.com\/ko\/noi-ban-naocl-10-12-tai-binh-duong-2\/#3_Loc_Thien_%E2%80%94_Nha_cung_cap_NaOCl_10%E2%80%9312_tai_Binh_Duong\" title=\"3. L\u1ed9c Thi\u00ean \u2014 Nh\u00e0 cung c\u1ea5p NaOCl 10\u201312% t\u1ea1i B\u00ecnh D\u01b0\u01a1ng\">3. L\u1ed9c Thi\u00ean \u2014 Nh\u00e0 cung c\u1ea5p NaOCl 10\u201312% t\u1ea1i B\u00ecnh D\u01b0\u01a1ng<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-4\" href=\"https:\/\/hoachatlocthien.com\/ko\/noi-ban-naocl-10-12-tai-binh-duong-2\/#4_Luu_y_khi_su_dung_luu_kho_NaOCl_10%E2%80%9312\" title=\"4. L\u01b0u \u00fd khi s\u1eed d\u1ee5ng &#038; l\u01b0u kho NaOCl 10\u201312%\">4. L\u01b0u \u00fd khi s\u1eed d\u1ee5ng &#038; l\u01b0u kho NaOCl 10\u201312%<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-5\" href=\"https:\/\/hoachatlocthien.com\/ko\/noi-ban-naocl-10-12-tai-binh-duong-2\/#Lien_he_Hoa_Chat_Loc_Thien\" title=\"Lien he Hoa Chat Loc Thien\">Lien he Hoa Chat Loc Thien<\/a><\/li><li class='ez-toc-page-1 ez-toc-heading-level-2'><a class=\"ez-toc-link ez-toc-heading-6\" href=\"https:\/\/hoachatlocthien.com\/ko\/noi-ban-naocl-10-12-tai-binh-duong-2\/#FAQ\" title=\"FAQ\">FAQ<\/a><\/li><\/ul><\/nav><\/div>\n<h2><span class=\"ez-toc-section\" id=\"1_Tieu_chuan_NaOCl_10%E2%80%9312_cong_nghiep\"><\/span>1. Ti\u00eau chu\u1ea9n NaOCl 10\u201312% c\u00f4ng nghi\u1ec7p<span class=\"ez-toc-section-end\"><\/span><\/h2>\n<table class='specs'>\n<tr>\n<th>Ch\u1ec9 ti\u00eau<\/th>\n<th>Y\u00eau c\u1ea7u<\/th>\n<\/tr>\n<tr>\n<td>Cl ho\u1ea1t \u0111\u1ed9ng (Cl available)<\/td>\n<td>10\u201312%<\/td>\n<\/tr>\n<tr>\n<td>NaOH d\u01b0<\/td>\n<td>0,5\u20131,5%<\/td>\n<\/tr>\n<tr>\n<td>NaCl<\/td>\n<td>\u2264 18%<\/td>\n<\/tr>\n<tr>\n<td>Fe<\/td>\n<td>\u2264 1 ppm<\/td>\n<\/tr>\n<tr>\n<td>T\u1ec9 tr\u1ecdng<\/td>\n<td>~ 1,20 g\/mL<\/td>\n<\/tr>\n<\/table>\n<\/section>\n<section id=\"ung-dung\">\n<h2><span class=\"ez-toc-section\" id=\"2_Ung_dung_NaOCl_10%E2%80%9312_tai_Binh_Duong\"><\/span>2. \u1ee8ng d\u1ee5ng NaOCl 10\u201312% t\u1ea1i B\u00ecnh D\u01b0\u01a1ng<span class=\"ez-toc-section-end\"><\/span><\/h2>\n<ul>\n<li>Kh\u1eed tr\u00f9ng n\u01b0\u1edbc c\u1ea5p KCN.<\/li>\n<li>Kh\u1eed tr\u00f9ng n\u01b0\u1edbc th\u1ea3i sau x\u1eed l\u00fd sinh h\u1ecdc.<\/li>\n<li>T\u1ea9y tr\u1eafng v\u1ea3i cotton, s\u1ee3i pha t\u1ea1i c\u00e1c nh\u00e0 m\u00e1y d\u1ec7t nhu\u1ed9m.<\/li>\n<li>Kh\u1eed tr\u00f9ng \u0111\u01b0\u1eddng \u1ed1ng nh\u00e0 m\u00e1y th\u1ef1c ph\u1ea9m, \u0111\u1ed3 u\u1ed1ng.<\/li>\n<\/ul>\n<\/section>\n<figure style=\"margin:18px 0;text-align:center;\"><img decoding=\"async\" class=\"thumb lazyload\" data-src=\"https:\/\/hoachatlocthien.com\/wp-content\/uploads\/2023\/12\/nuoc-Javen.webp\" alt=\"n\u01b0\u1edbc Javen 10%\" src=\"data:image\/gif;base64,R0lGODlhAQABAAAAACH5BAEKAAEALAAAAAABAAEAAAICTAEAOw==\"><figcaption class=\"meta\">n\u01b0\u1edbc Javen 10%<\/figcaption><\/figure>\n<section id=\"loc-thien\">\n<h2><span class=\"ez-toc-section\" id=\"3_Loc_Thien_%E2%80%94_Nha_cung_cap_NaOCl_10%E2%80%9312_tai_Binh_Duong\"><\/span>3. L\u1ed9c Thi\u00ean \u2014 Nh\u00e0 cung c\u1ea5p NaOCl 10\u201312% t\u1ea1i B\u00ecnh D\u01b0\u01a1ng<span class=\"ez-toc-section-end\"><\/span><\/h2>\n<ul>\n<li>H\u00e0ng t\u01b0\u01a1i, ra x\u01b0\u1edfng t\u1edbi kh\u00e1ch trong v\u00f2ng 24 gi\u1edd.<\/li>\n<li>Phi\u1ebfu test n\u1ed3ng \u0111\u1ed9 Cl ho\u1ea1t \u0111\u1ed9ng cho t\u1eebng l\u00f4.<\/li>\n<li>IBC 1.000L PE chuy\u00ean d\u1ee5ng c\u00f3 l\u1ed7 tho\u00e1t O2.<\/li>\n<li>\u0110\u1ed9i xe giao t\u1eadn kho kh\u00e1ch h\u00e0ng KCN B\u00ecnh D\u01b0\u01a1ng.<\/li>\n<\/ul>\n<\/section>\n<section id=\"luu-y\">\n<h2><span class=\"ez-toc-section\" id=\"4_Luu_y_khi_su_dung_luu_kho_NaOCl_10%E2%80%9312\"><\/span>4. L\u01b0u \u00fd khi s\u1eed d\u1ee5ng &#038; l\u01b0u kho NaOCl 10\u201312%<span class=\"ez-toc-section-end\"><\/span><\/h2>\n<ul>\n<li>B\u1ea3o qu\u1ea3n 15\u201325\u00b0C, tr\u00e1nh n\u1eafng v\u00e0 ngu\u1ed3n nhi\u1ec7t.<\/li>\n<li>B\u1ed3n HDPE c\u00f3 van tho\u00e1t O2, kh\u00f4ng \u0111\u1eady k\u00edn ho\u00e0n to\u00e0n.<\/li>\n<li>Tuy\u1ec7t \u0111\u1ed1i kh\u00f4ng tr\u1ed9n v\u1edbi axit (HCl, H2SO4) \u2013 sinh kh\u00ed Cl2 \u0111\u1ed9c.<\/li>\n<li>N\u1ed3ng \u0111\u1ed9 gi\u1ea3m theo th\u1eddi gian \u2013 n\u00ean \u0111\u1eb7t mua \u0111\u1ee7 d\u00f9ng trong 1\u20132 th\u00e1ng.<\/li>\n<\/ul>\n<\/section>\n<section id=\"lien-he\">\n<h2><span class=\"ez-toc-section\" id=\"Lien_he_Hoa_Chat_Loc_Thien\"><\/span>Lien he Hoa Chat Loc Thien<span class=\"ez-toc-section-end\"><\/span><\/h2>\n<p>Doi ngu ky thuat <strong>Hoa Chat Loc Thien<\/strong> san sang ho tro doanh nghiep.<\/p>\n<ul>\n<li>Hotline: <a href=\"tel:0979891929\">0979 89 1929<\/a><\/li>\n<li>Email: <a href=\"mailto:locthien@locthien.vn\">locthien@locthien.vn<\/a><\/li>\n<li>Website: <a href=\"https:\/\/hoachatlocthien.com\/\">hoachatlocthien.com\/<\/a><\/li>\n<\/ul>\n<\/section>\n<section id=\"faq\" class=\"faq\">\n<h2><span class=\"ez-toc-section\" id=\"FAQ\"><\/span>FAQ<span class=\"ez-toc-section-end\"><\/span><\/h2>\n<ol>\n<li><strong>Mua NaOCl 10-12% t\u1ea1i B\u00ecnh D\u01b0\u01a1ng \u1edf \u0111\u00e2u nhanh?<\/strong><br \/>L\u1ed9c Thi\u00ean c\u00f3 kho NaOCl 10-12% t\u1ea1i B\u00ecnh D\u01b0\u01a1ng, h\u00e0ng t\u01b0\u01a1i giao trong ng\u00e0y t\u1ea1i c\u00e1c KCN S\u00f3ng Th\u1ea7n, M\u1ef9 Ph\u01b0\u1edbc, Vi\u1ec7t H\u01b0\u01a1ng. Hotline 0979 89 1929.<\/li>\n<li><strong>NaOCl 10-12% b\u1ea3o qu\u1ea3n t\u1ed1i \u0111a bao l\u00e2u?<\/strong><br \/>Trong \u0111i\u1ec1u ki\u1ec7n 15-25\u00b0C, tr\u00e1nh n\u1eafng, NaOCl 10-12% gi\u1ea3m kho\u1ea3ng 1-2% n\u1ed3ng \u0111\u1ed9 Cl\/th\u00e1ng. N\u00ean \u0111\u1eb7t mua \u0111\u1ee7 d\u00f9ng trong 1-2 th\u00e1ng \u0111\u1ec3 gi\u1eef ch\u1ea5t l\u01b0\u1ee3ng.<\/li>\n<li><strong>Li\u1ec1u d\u00f9ng NaOCl 10-12% cho kh\u1eed tr\u00f9ng n\u01b0\u1edbc c\u1ea5p?<\/strong><br \/>Cl d\u01b0 sau kh\u1eed tr\u00f9ng 0,2-0,5 mg\/L (theo QCVN n\u01b0\u1edbc s\u1ea1ch). Li\u1ec1u ch\u00e2m c\u1ee5 th\u1ec3 ph\u1ee5 thu\u1ed9c nhu c\u1ea7u Cl c\u1ee7a n\u01b0\u1edbc, th\u01b0\u1eddng 1-3 mL NaOCl 10-12% m\u1ed7i m\u00b3 n\u01b0\u1edbc.<\/li>\n<li><strong>NaOCl 10-12% c\u00f3 an to\u00e0n cho th\u1ef1c ph\u1ea9m kh\u00f4ng?<\/strong><br \/>NaOCl industrial-grade 10-12% c\u00f3 th\u1ec3 d\u00f9ng kh\u1eed tr\u00f9ng \u0111\u01b0\u1eddng \u1ed1ng, sau \u0111\u00f3 r\u1eeda l\u1ea1i b\u1eb1ng n\u01b0\u1edbc s\u1ea1ch. Kh\u00f4ng d\u00f9ng \u0111\u1ec3 r\u1eeda th\u1ef1c ph\u1ea9m tr\u1ef1c ti\u1ebfp \u1edf n\u1ed3ng \u0111\u1ed9 cao.<\/li>\n<li><strong>L\u1ed9c Thi\u00ean c\u00f3 giao IBC NaOCl t\u1ea1i B\u00ecnh D\u01b0\u01a1ng ngay trong ng\u00e0y kh\u00f4ng?<\/strong><br \/>C\u00f3. \u0110\u1ed9i xe L\u1ed9c Thi\u00ean giao IBC 1.000L NaOCl 10-12% trong v\u00f2ng v\u00e0i gi\u1edd t\u1ea1i c\u00e1c KCN B\u00ecnh D\u01b0\u01a1ng khi \u0111\u1eb7t h\u00e0ng tr\u01b0\u1edbc 9h s\u00e1ng.<\/li>\n<\/ol>\n<\/section>\n<\/article>\n<p><script type=\"application\/ld+json\">\n{\n  \"@context\": \"https:\/\/schema.org\",\n  \"@graph\": [\n    {\n      \"@type\": \"Organization\",\n      \"@id\": \"https:\/\/hoachatlocthien.com\/#org\",\n      \"name\": \"Hoa Chat Loc Thien\",\n      \"url\": \"https:\/\/hoachatlocthien.com\/\",\n      \"logo\": \"https:\/\/hoachatlocthien.com\/wp-content\/uploads\/2025\/02\/logo-locthien.png\",\n      \"telephone\": \"+84979891929\",\n      \"email\": \"locthien@locthien.vn\"\n    },\n    {\n      \"@type\": \"BreadcrumbList\",\n      \"@id\": \"https:\/\/hoachatlocthien.com\/noi-ban-naocl-10-12-tai-binh-duong\/#breadcrumb\",\n      \"itemListElement\": [\n        {\n          \"@type\": \"ListItem\",\n          \"position\": 1,\n          \"name\": \"Trang chu\",\n          \"item\": \"https:\/\/hoachatlocthien.com\/\"\n        },\n        {\n          \"@type\": \"ListItem\",\n          \"position\": 2,\n          \"name\": \"H\u00f3a ch\u1ea5t x\u1eed l\u00fd n\u01b0\u1edbc\",\n          \"item\": \"https:\/\/hoachatlocthien.com\/kien-thuc-hoa-chat\/\"\n        },\n        {\n          \"@type\": \"ListItem\",\n          \"position\": 3,\n          \"name\": \"N\u01a1i B\u00e1n NaOCl 10\u201312% (Javen C\u00f4ng Nghi\u1ec7p) T\u1ea1i B\u00ecnh D\u01b0\u01a1ng\",\n          \"item\": \"https:\/\/hoachatlocthien.com\/noi-ban-naocl-10-12-tai-binh-duong\/\"\n        }\n      ]\n    },\n    {\n      \"@type\": \"Article\",\n      \"@id\": \"https:\/\/hoachatlocthien.com\/noi-ban-naocl-10-12-tai-binh-duong\/#article\",\n      \"headline\": \"N\u01a1i B\u00e1n NaOCl 10\u201312% (Javen C\u00f4ng Nghi\u1ec7p) T\u1ea1i B\u00ecnh D\u01b0\u01a1ng\",\n      \"description\": \"NaOCl 10\u201312% (Javen c\u00f4ng nghi\u1ec7p) l\u00e0 ch\u1ea5t kh\u1eed tr\u00f9ng v\u00e0 t\u1ea9y tr\u1eafng ph\u1ed5 bi\u1ebfn. N\u01a1i b\u00e1n NaOCl 10\u201312% t\u1ea1i B\u00ecnh D\u01b0\u01a1ng \u2014 L\u1ed9c Thi\u00ean giao trong ng\u00e0y t\u1ea1i c\u00e1c KCN.\",\n      \"image\": \"https:\/\/hoachatlocthien.com\/wp-content\/uploads\/2023\/12\/Javen.webp\",\n      \"datePublished\": \"2026-05-06T08:00:00+07:00\",\n      \"dateModified\": \"2026-05-06T08:00:00+07:00\",\n      \"author\": {\n        \"@type\": \"Organization\",\n        \"@id\": \"https:\/\/hoachatlocthien.com\/#org\",\n        \"name\": \"Hoa Chat Loc Thien\"\n      },\n      \"publisher\": {\n        \"@type\": \"Organization\",\n        \"@id\": \"https:\/\/hoachatlocthien.com\/#org\"\n      },\n      \"mainEntityOfPage\": {\n        \"@type\": \"WebPage\",\n        \"@id\": \"https:\/\/hoachatlocthien.com\/noi-ban-naocl-10-12-tai-binh-duong\/\"\n      },\n      \"articleSection\": [\n        \"H\u00f3a ch\u1ea5t x\u1eed l\u00fd n\u01b0\u1edbc\",\n        \"Javen\"\n      ],\n      \"keywords\": [\n        \"NaOCl 10-12%\",\n        \"Javen B\u00ecnh D\u01b0\u01a1ng\",\n        \"Javen c\u00f4ng nghi\u1ec7p\",\n        \"NaOCl B\u00ecnh D\u01b0\u01a1ng\",\n        \"Javen 12%\"\n      ]\n    },\n    {\n      \"@type\": \"FAQPage\",\n      \"@id\": \"https:\/\/hoachatlocthien.com\/noi-ban-naocl-10-12-tai-binh-duong\/#faq-schema\",\n      \"mainEntity\": [\n        {\n          \"@type\": \"Question\",\n          \"name\": \"Mua NaOCl 10-12% t\u1ea1i B\u00ecnh D\u01b0\u01a1ng \u1edf \u0111\u00e2u nhanh?\",\n          \"acceptedAnswer\": {\n            \"@type\": \"Answer\",\n            \"text\": \"L\u1ed9c Thi\u00ean c\u00f3 kho NaOCl 10-12% t\u1ea1i B\u00ecnh D\u01b0\u01a1ng, h\u00e0ng t\u01b0\u01a1i giao trong ng\u00e0y t\u1ea1i c\u00e1c KCN S\u00f3ng Th\u1ea7n, M\u1ef9 Ph\u01b0\u1edbc, Vi\u1ec7t H\u01b0\u01a1ng. Hotline 0979 89 1929.\"\n          }\n        },\n        {\n          \"@type\": \"Question\",\n          \"name\": \"NaOCl 10-12% b\u1ea3o qu\u1ea3n t\u1ed1i \u0111a bao l\u00e2u?\",\n          \"acceptedAnswer\": {\n            \"@type\": \"Answer\",\n            \"text\": \"Trong \u0111i\u1ec1u ki\u1ec7n 15-25\u00b0C, tr\u00e1nh n\u1eafng, NaOCl 10-12% gi\u1ea3m kho\u1ea3ng 1-2% n\u1ed3ng \u0111\u1ed9 Cl\/th\u00e1ng. N\u00ean \u0111\u1eb7t mua \u0111\u1ee7 d\u00f9ng trong 1-2 th\u00e1ng \u0111\u1ec3 gi\u1eef ch\u1ea5t l\u01b0\u1ee3ng.\"\n          }\n        },\n        {\n          \"@type\": \"Question\",\n          \"name\": \"Li\u1ec1u d\u00f9ng NaOCl 10-12% cho kh\u1eed tr\u00f9ng n\u01b0\u1edbc c\u1ea5p?\",\n          \"acceptedAnswer\": {\n            \"@type\": \"Answer\",\n            \"text\": \"Cl d\u01b0 sau kh\u1eed tr\u00f9ng 0,2-0,5 mg\/L (theo QCVN n\u01b0\u1edbc s\u1ea1ch). Li\u1ec1u ch\u00e2m c\u1ee5 th\u1ec3 ph\u1ee5 thu\u1ed9c nhu c\u1ea7u Cl c\u1ee7a n\u01b0\u1edbc, th\u01b0\u1eddng 1-3 mL NaOCl 10-12% m\u1ed7i m\u00b3 n\u01b0\u1edbc.\"\n          }\n        },\n        {\n          \"@type\": \"Question\",\n          \"name\": \"NaOCl 10-12% c\u00f3 an to\u00e0n cho th\u1ef1c ph\u1ea9m kh\u00f4ng?\",\n          \"acceptedAnswer\": {\n            \"@type\": \"Answer\",\n            \"text\": \"NaOCl industrial-grade 10-12% c\u00f3 th\u1ec3 d\u00f9ng kh\u1eed tr\u00f9ng \u0111\u01b0\u1eddng \u1ed1ng, sau \u0111\u00f3 r\u1eeda l\u1ea1i b\u1eb1ng n\u01b0\u1edbc s\u1ea1ch. Kh\u00f4ng d\u00f9ng \u0111\u1ec3 r\u1eeda th\u1ef1c ph\u1ea9m tr\u1ef1c ti\u1ebfp \u1edf n\u1ed3ng \u0111\u1ed9 cao.\"\n          }\n        },\n        {\n          \"@type\": \"Question\",\n          \"name\": \"L\u1ed9c Thi\u00ean c\u00f3 giao IBC NaOCl t\u1ea1i B\u00ecnh D\u01b0\u01a1ng ngay trong ng\u00e0y kh\u00f4ng?\",\n          \"acceptedAnswer\": {\n            \"@type\": \"Answer\",\n            \"text\": \"C\u00f3. \u0110\u1ed9i xe L\u1ed9c Thi\u00ean giao IBC 1.000L NaOCl 10-12% trong v\u00f2ng v\u00e0i gi\u1edd t\u1ea1i c\u00e1c KCN B\u00ecnh D\u01b0\u01a1ng khi \u0111\u1eb7t h\u00e0ng tr\u01b0\u1edbc 9h s\u00e1ng.\"\n          }\n        }\n      ]\n    }\n  ]\n}\n<\/script><\/p>\n","protected":false},"excerpt":{"rendered":"<p>NaOCl 10\u201312% (Javen c\u00f4ng nghi\u1ec7p) l\u00e0 ch\u1ea5t kh\u1eed tr\u00f9ng v\u00e0 t\u1ea9y tr\u1eafng ph\u1ed5 bi\u1ebfn. N\u01a1i b\u00e1n NaOCl 10\u201312% t\u1ea1i B\u00ecnh D\u01b0\u01a1ng \u2014 L\u1ed9c Thi\u00ean giao trong ng\u00e0y t\u1ea1i c\u00e1c KCN.<\/p>","protected":false},"author":6,"featured_media":0,"comment_status":"closed","ping_status":"closed","sticky":false,"template":"","format":"standard","meta":{"_acf_changed":false,"footnotes":""},"categories":[1234],"tags":[1383,1381,1283,1282,1382],"class_list":["post-9044","post","type-post","status-publish","format-standard","hentry","category-hoa-chat-xu-ly-nuoc","tag-javen-12","tag-javen-binh-duong","tag-javen-cong-nghiep","tag-naocl-10-12","tag-naocl-binh-duong"],"acf":[],"_links":{"self":[{"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/posts\/9044","targetHints":{"allow":["GET"]}}],"collection":[{"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/posts"}],"about":[{"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/types\/post"}],"author":[{"embeddable":true,"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/users\/6"}],"replies":[{"embeddable":true,"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/comments?post=9044"}],"version-history":[{"count":1,"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/posts\/9044\/revisions"}],"predecessor-version":[{"id":9077,"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/posts\/9044\/revisions\/9077"}],"wp:attachment":[{"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/media?parent=9044"}],"wp:term":[{"taxonomy":"category","embeddable":true,"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/categories?post=9044"},{"taxonomy":"post_tag","embeddable":true,"href":"https:\/\/hoachatlocthien.com\/ko\/wp-json\/wp\/v2\/tags?post=9044"}],"curies":[{"name":"wp","href":"https:\/\/api.w.org\/{rel}","templated":true}]}}