FeSO4 Chemical Quality and Comprehensive Applications

Technical Specifications FeSO4 — Iron(II) Sulfate

Specifications Anhydrous Form Hydrated Form (FeSO₄·7H₂O)

Chemical Name Iron(II) Sulfate
CAS Number7720-78-7
Iron(II) sulfate, Iron(II) sulfate heptahydrate
Molar mass 151.91 g/mol 278.01 g/mol
Fe²⁺ content ≥ 30%; ≥ 19.5%
Colors White Gray Cyan (teal)
Solubility (20°C) 26.3 g/100ml water
Packaging specifications: 25kg, 50kg bags; 1,000L IBC tanks
TCVN / GHS / ISO 9001 Standards

FeSO4 Used in Agriculture & Dyeing — Unique Angle
Beyond water treatment, FeSO4 has two specific applications that many suppliers do not mention:

Iron micronutrient (Fe-EDDHA substitute): FeSO₄ directly supplies Fe²⁺ to plants suffering from yellowing leaves (iron chlorosis). Dilute to a concentration of 0.1–0.5% and apply as a root drench or foliar spray. Commonly used in hydroponic vegetable cultivation, ornamental plants, and dragon fruit.
Color fixing in dyeing (mordanting): FeSO₄ is used as a mordant in natural and synthetic dyeing processes, helping the dye adhere firmly to cotton and linen fibers. The recommended ratio is 2–5% based on the weight of the fabric.
Electroplating wastewater treatment: Reduce Cr(VI) to Cr(III) according to QCVN 40:2011/BTNMT before precipitation. The FeSO4 : Cr(VI) ratio is 3:1 (molar ratio) at pH 2–3.

Comparison: FeSO4 vs. FeCl3 vs. PAC — Choose the Right Chemical

Criteria FeSO4 FeCl3 PAC

Active ions
Optimal pH: 8–9 (after oxidation); 5–9; 6–9
Cloudy water coagulant (requires oxidation)
Phosphorus Removal
Agriculture (iron fertilizer)⭐⭐⭐⭐⭐❌❌
Dyeing (mordant)
Hexavalent Chromium Removal
Lowest price Average Higher
Mud color generated Black (Fe²⁺→Fe³⁺) Reddish-brown Ivory

Standards & Shipping Documents

Certificate of Analysis Graded by batch — Fe²⁺ ≥19.5%, SO₄²⁻, As/Pb/Cd impurities
MSDS/SDS (Safety Data Sheet): GHS Rev.9 — hazard classification, EUH032 (releases H₂S gas on contact with acid)
Origin/Quality Accompanied by each shipment
Wastewater standards QCVN 40:2011/BTNMT Column A - Supporting businesses to calculate the required dose of FeSO4

Warehouse & Shipping Industrial Park — Loc Thien
Lộc Thiên has 3 strategic warehouses Ensure delivery of FeSO4 today

🏭 Ho Chi Minh City Warehouse — Delivery within the city and to Tan Binh, Tan Phu, Binh Chanh industrial parks
🏭 Binh Duong Warehouse — VSIP 1, VSIP 2, My Phuoc 1-3, Song Than Industrial Park Transportation
🏭 Dong Nai Warehouse — Nhon Trach 1–6, Amata, Long Thanh, Bien Hoa 1–2 Industrial Parks

Order before 2 PM → same-day delivery. 5–30 ton tankers. Pumping into on-site tanks supported.

Safe Use of FeSO4

GHS Signal Word: Warning
Eye/skin irritation: Wear safety glasses and gloves when operating.
Do not come into contact with strong acids EUH032: Contact with acids liberates very toxic gas
Storage: Store in a cool, dry, well-ventilated place, away from moisture — FeSO4 is easily oxidized to yellow Fe₂(SO4)₃.
Dosage for electroplating wastewater treatment: Input Cr(VI) check → calculate by 3:1 molar ratio → adjust pH after reduction