Industrial Hydrochloric Acid 32%–35% (Muriatic Acid) – Steel Pickling & DI Water Treatment Bulk 5–30 Ton Tankers

Industrial Hydrochloric Acid 32%–35% (Muriatic Acid) – Steel Pickling & DI Water Treatment Bulk 5–30 Ton Tankers

Loc Thien Chemical is a Industrial Chemical Bulk Supplier of Industrial Hydrochloric Acid 32% & 35% (HCl, CAS 7647-01-0) in Vietnam. Heavy-duty rubber/FRP lined 5–30-ton road tankers. Ideal for steel pickling, DI resin regeneration, and WWTP neutralization. 15-minute quotation. Hotline: +84 979 891 929.

Call 0979 891 929 Request a quote 💬 Zalo: 0979 891 929

Industrial Hydrochloric Acid 32% and 35% (Muriatic Acid, Aqueous Hydrogen Chloride) (CAS 7647-01-0, MW 36.46 g/mol) is a heavy-duty inorganic acid solution supplied by Loc Thien Chemical as a Industrial Chemical Bulk Supplier to manufacturing plants across Vietnam. Presenting a density of 1.159 g/cm³ (32% grade) and 1.174 g/cm³ (35% grade), this clear to pale yellow fuming liquid is extensively utilized for continuous steel wire/sheet pickling, ion-exchange resin regeneration in DI water plants, and automated wastewater neutralization. Loc Thien Chemical operates a specialized fleet of 5–30-ton rubber/FRP-lined chemical road tankers, guaranteeing continuous deliveries across Binh Duong, Dong Nai, Long An, Bac Ninh, and Hai Phong with a guaranteed 15-minute RFQ turnaround.

Loc Thien Chemical maintains direct direct bulk supply channels with Vietnam's largest chlor-alkali complexes, securing thousands of tons of high-grade technical HCl monthly. Every consignment is supported by comprehensive lot-specific COAs, TDS, and bilingual SDS/MSDS complying with Vietnamese environmental standard QCVN 40:2025/BTNMT.

Hydrochloric Acid 32% & 35% Technical Specifications

Loc Thien's industrial hydrochloric acid meets Vietnamese technical standard TCCS 01:2018/LT and international standard ASTM E1146.

ParameterHCl 32% SpecificationHCl 35% SpecificationTest Method
Chemical NameAqueous Hydrochloric Acid SolutionIUPAC / CAS Nomenclature
Chemical Formula & MWHCl (36.46 g/mol)Structural Chemistry
CAS Registry Number7647-01-0CAS Registry
UN Number & Hazard ClassUN 1789, Class 8 Corrosive Liquid, Packing Group IIDOT / IMDG Rules
HCl Concentration32.0% ± 1.0%35.0% ± 1.0%Acid-Base Titration
AppearanceClear, colorless to light yellow fuming liquidVisual Inspection
Density (at 20°C)1.154 – 1.164 g/cm³1.169 – 1.179 g/cm³Hydrometer / ASTM D1298
Specific Gravity / Baumé19.5° – 20.5° Bé21.0° – 22.0° BéBaumé Hydrometry
Free Chlorine (Cl₂)≤ 50 ppm≤ 80 ppmIodometric Titration
Iron (Fe) Content≤ 5 ppm (High purity)≤ 10 ppmICP-OES / AAS
Packaging & Delivery30L Cans, 250kg Drums, 1,000L IBCs, 5–30-ton Lined TankersAcid-Resistant Dedicated Units
Industrial Hydrochloric Acid 32%–35% (Muriatic Acid) – Steel Pickling & DI Water Treatment Bulk 5–30 Ton Tankers
Actual industrial field deployment, automated dosing system, and 5–30-ton bulk tanker logistics at Loc Thien Chemical.

Industrial Applications and Reaction Mechanisms

1. Continuous Steel Pickling and Oxide Scale Removal

Hydrochloric acid rapidly dissolves rust and mill scale (Fe₂O₃, Fe₃O₄, FeO) from hot-rolled carbon steel prior to electroplating, galvanizing, or cold drawing:

Fe₂O₃ + 6HCl → 2FeCl₃ + 3H₂O
Fe + 2HCl → FeCl₂ + H₂ ↑

Compared to sulfuric acid, hydrochloric pickling operates at lower temperatures, prevents hydrogen embrittlement, and delivers superior metallic surface brightness.

2. Demineralization Plant (DI/RO) Cation Resin Regeneration

Supplies high concentrations of hydrogen ions (H⁺) to displace accumulated calcium, magnesium, and sodium cations from exhausted strong acid cation (SAC) resin beds in electronics and pharmaceutical manufacturing.

EHS Safety Protocols and Fume Scrubber Requirements

🛑 Mandatory Wet Scrubber Venting for Concentrated HCl Vapors

Concentrated hydrochloric acid exhibits high vapor pressure, releasing pungent, corrosive hydrogen chloride fumes upon exposure to atmospheric moisture. Breather vents on storage tanks must be directly integrated with a packed-bed wet scrubber operating with circulating water or dilute caustic solution to prevent hazardous emissions exceeding OSHA/QCVN limits.

  • Storage Metallurgy: Concentrated HCl rapidly attacks carbon steel and all grades of stainless steel (including SUS304 and SUS316). Permissible construction materials are strictly limited to Fiber-Reinforced Plastic (Vinyl Ester FRP), HDPE, Polypropylene (PP), or Natural Rubber-Lined Steel.

⚡ Request Bulk Tanker Quotation (15-Minute Response)

Contact Loc Thien Chemical for contract pricing and scheduled bulk tanker deliveries of technical grade HCl 32% and 35%.

ZDHC MRSL Version 3.1 Conformance Level 1 — Hydrochloric Acid (HCl 32%–35%)

  • Official Documentation: ZDHC MRSL Version 3.1 Level 1 Conformance Summary Report (CSR) & Analytical Test Report
  • Issuing Body: TÜV Rheinland Vietnam Co., Ltd.
  • Certificate / Report Holder: LOC THIEN INVESTMENT DEVELOPMENT COMPANY LIMITED
  • Certificate / CSR No.: CSR #248162921-03 (22/10/2024) | Analytical Test Report No.: 248162921-03
  • Analytical Results: 3/3 Smart Testing substance groups PASS: Total Heavy Metal; Borate, zinc salt; Perboric acid, sodium salt

Loc Thien 9-Product ZDHC MRSL v3.1 Level 1 Portfolio: Includes 4 TÜV SÜD Level 1 Certificates (ZDHC1 127736 0001–0004: NaOH, H₂O₂, Na₂SO₄, Na₂CO₃) and 5 TÜV Rheinland Level 1 CSR & Analytical Test Reports (248162921-01–05: H₂SO₄, FeCl₂, HCl, Javel/NaOCl, PAC 31%). FDI textile and footwear manufacturers requiring official PDF dossiers with batch COA/SDS for ZDHC Gateway audits may request documentation here (15-minute response SLA).

Related products

WeChat B2B

Connect via WeChat B2B

Loc Thien Chemical — Direct Manufacturer & Industrial Chemical Supplier

Loc Thien Chemical Official WeChat B2B QR Code 0979891929

Scan QR code with WeChat on your phone

WeChat ID 0979891929

Tap the copy button above, then open WeChat and paste ID into Search to connect.

Direct Technical & Bulk Quotation Hotline: 📞 0979 891 929