High Purity Nitric Acid 68% (Korean Imported Grade) – Stainless Steel Passivation & Electronics (35kg Can/280kg Drum/IBC Supply)

High Purity Nitric Acid 68% (Korean Imported Grade) – Stainless Steel Passivation & Electronics (35kg Can/280kg Drum/IBC Supply)

Loc Thien Chemical is a Industrial Chemical Bulk Supplier of High Purity Nitric Acid 68% (HNO3, CAS 7697-37-2) imported from Korea. Density 1.41 g/cm³, essential for stainless steel passivation, pickling, and electroplating. Supplied in 35kg cans, 280kg drums, IBC tanks (no tankers). Hotline: +84 979 891 929.

Call 0979 891 929 Request a quote 💬 Zalo: 0979 891 929

High Purity Nitric Acid 68% (Korean Imported Technical Grade, Aqua Fortis) (CAS 7697-37-2, MW 63.01 g/mol) is a premium inorganic strong oxidizing acid imported directly from leading South Korean chemical manufacturers by Loc Thien Chemical as a Industrial Chemical Bulk Supplier. With a density of 1.410 g/cm³ at 20°C, this colorless to pale straw-colored fuming liquid is critical for stainless steel surface pickling, forming durable passive chromium oxide films (Cr₂O₃), semiconductor copper etching, and advanced electroplating. [Strict Logistics Compliance] Due to severe oxidizing hazards and imported cargo integrity, road tanker delivery is strictly prohibited for this product; shipments are supplied exclusively in original 35kg cans, 280kg drums, and 1,400kg IBC containers. Loc Thien Chemical ensures a swift 15-minute quotation turnaround.

Loc Thien Chemical provides genuine manufacturer Certificates of Analysis (COA) and import customs clearance declarations with every lot, maintaining extensive reserve inventories across 6 strategically located logistics hubs in Vietnam.

Nitric Acid 68% Korean Grade Specifications

Loc Thien's imported Korean nitric acid 68% conforms to KS M 1108 and ASTM technical standards for high-purity surface engineering.

ParameterTechnical SpecificationTest Method
Chemical NameNitric Acid 68% (Korean Origin)IUPAC / CAS Nomenclature
Chemical Formula & MWHNO₃ (63.01 g/mol)Structural Chemistry
CAS Registry Number7697-37-2CAS Registry
UN Number & Hazard ClassUN 2031, Class 8 Corrosive + Sub-risk 5.1 OxidizerIMDG / IATA Regulations
HNO₃ Concentration68.0% ± 0.5%Acid-Base Titration
AppearanceClear, colorless to slightly yellowish fuming liquidVisual Inspection
Density (at 20°C)1.405 – 1.415 g/cm³Hydrometer / ASTM D1298
Nitrous Acid (HNO₂)≤ 0.01%Potassium Permanganate Titration
Chloride (Cl) Impurities≤ 0.5 ppm (Ultra-trace controlled)Ion Chromatography
Sulfate (SO₄) Impurities≤ 1.0 ppmTurbidimetry
Iron (Fe) Content≤ 0.5 ppm (Electronics grade)ICP-MS Instrument Analysis
Packaging & Dispatch Units35kg Cans, 280kg Drums, 1,400kg IBCs (No Tankers)UV-Shielded Dedicated Poly Units
High Purity Nitric Acid 68% (Korean Imported Grade) – Stainless Steel Passivation & Electronics (35kg Can/280kg Drum/IBC Supply)
Actual industrial field deployment, automated dosing system, and 5–30-ton bulk tanker logistics at Loc Thien Chemical.

Surface Passivation Mechanisms and Photodecomposition Safety

1. Stainless Steel Passivation Chemistry

Nitric acid oxidizes surface free iron, selectively dissolving non-noble contaminants while promoting the formation of an ultra-thin, highly resistant chromium oxide passive layer:

2Fe + 6HNO₃ → 2Fe(NO₃)₃ + 3H₂ ↑

2. Photolytic Decomposition and Storage Protocol

When exposed to sunlight or heat, nitric acid undergoes photolytic degradation, yielding brown, toxic nitrogen dioxide gas (NO₂):

4HNO₃ ──[hnu, Δ]──> 4NO₂ ↑ + O₂ ↑ + 2H₂O

Keep containers tightly closed in dark, well-ventilated, temperature-controlled chemical warehouses away from organic solvents, oils, and combustible reducing agents.

⚡ Request Korean Nitric Acid 68% Spot Pricing (15-Minute Turnaround)

Contact Loc Thien Chemical for immediate dispatch of 35kg cans, 280kg drums, or IBC totes with full analytical certification.

Related products

WeChat B2B

Connect via WeChat B2B

Loc Thien Chemical — Direct Manufacturer & Industrial Chemical Supplier

Loc Thien Chemical Official WeChat B2B QR Code 0979891929

Scan QR code with WeChat on your phone

WeChat ID 0979891929

Tap the copy button above, then open WeChat and paste ID into Search to connect.

Direct Technical & Bulk Quotation Hotline: 📞 0979 891 929