Liquid PAC (Polyaluminium Chloride) — Al₂O₃ Coagulation...: Liquid PAC (CAS 1327-41-9) with 10–17% Al2O3: a dust-free coagulant that is easy to pump and dose for plant wastewater. Loc Thien, hotline 0979 891 929 Supplied in bulk from 6 industrial park warehouses across Vietnam (Ba Ria - Vung Tau, Dong Nai, Binh Duong, Da Nang, Can Tho, Bac Ninh) via licensed 5–30-ton hazmat tankers and 1,000L IBC totes (3,000+ MT/month capacity), complete with batch COA, 16-section GHS SDS, and EPE customs support. Contact hotline 0979 891 929 for detailed delivery procedures and a technical quotation within 15 minutes.

Liquid PAC (Polyaluminium Chloride) — Al₂O₃ Coagulation 10-17% | Delivery to Industrial Parks

What Is Liquid PAC (Polyaluminium Chloride)? What Is the Al₂O₃ Percentage?

Liquid PAC (Polyaluminium Chloride, CAS 1327-41-9) is a liquid coagulation agent, with Al₂O₃ content ranging from 10% to 17%. It is easy to pump and dose, produces no dust—offering significant advantages over powdered PAC (Polyaluminium Chloride) in water treatment plants and Wastewater Treatment facilities. Loc Thien supplies liquid PAC (Polyaluminium Chloride) that meets QCVN 01:2009/BYT standards for potable water, complete with CoA, CO, CQ, and MSDS documentation.

Comparison of Liquid PAC (Polyaluminium Chloride) — Powdered PAC (Polyaluminium Chloride) — Aluminium Sulfate

Criteria
Liquid PAC (10-17%)
Powdered PAC (28-31%)
Aluminium Sulfate

Form
Pale
yellow solution White
powder/granules White crystals/powder

Easy to dose via pump
✅ Very easy (direct pumping)
⚠️ Must be pre-diluted
⚠️ Must be pre-diluted

Dust Generation (Occupational
Safety) ✅ Dust-free
❌ Dust
present ❌ Dust present

Turbidity effectiveness (NTU)
: Good from 10–500 NTU
; Good from 10–1,000 NTU
; Average, >100 NTU

Operating
pH range 5.0 – 9.0
5.0 – 9.0
6.5 – 7.5

CAS Number
1327-41-9
1327-41-9
10043-01-3

Technical Specifications Liquid PAC (Polyaluminium Chloride) (CAS 1327-41-9)

Characteristics
Liquid PAC (Polyaluminium Chloride) 10%
Liquid PAC (Polyaluminium Chloride) 17%

Al₂O₃ Content / Purity (%)
≥ 10
≥ 17

Density (g/cm³)
1.10 – 1.15
1.20 – 1.25

pH (1% solution)
3.5 – 5.0
3.5 – 5.0

Insoluble Impurities (%)
≤ 0.1
≤ 0.1

Drinking
Water Certification QCVN 01:2009/BYT
QCVN 01:2009/BYT

Accompanying
Documentation: CoA, CO, CQ, MSDS
CoA, CO, CQ, MSDS

Dosage of Liquid PAC (Polyaluminium Chloride) Based on Water Turbidity

Low turbidity water (below 50 NTU): 1–3 mg/L liquid PAC (Polyaluminium Chloride) 10%.
Moderately turbid water (50–200 NTU): 3–8 mg/L liquid PAC (Polyaluminium Chloride) 10–17%.
High turbidity water (above 200 NTU): 8–15 mg/L liquid PAC (Polyaluminium Chloride) 17%, combined with a coagulation-enhancing polymer.
Directly dose into the rapid mixing point. No further dilution with liquid PAC (Polyaluminium Chloride) is required.

Applications of Liquid PAC (Polyaluminium Chloride) by Industry

Water Supply Treatment and Industrial Water Treatment: Rapid coagulation of organic and inorganic impurities. Meets QCVN 01:2009/BYT standards.
Industrial Wastewater Treatment: VSIP Industrial Park, Nhon Trach Industrial Park, Amata Industrial Park — delivery, support for dosing pump systems.
Textile Dyeing, Pulp & Paper Industries: Removes color, suspended solids, and improves COD/BOD.
Aquaculture: Clarifies ponds and rapidly reduces turbidity.

Why Choose Loc Thien as Your Liquid PAC (Polyaluminium Chloride) Partner?

Full Documentation: Each shipment includes a Certificate of Analysis (CoA), Certificate of Origin (CO), Certificate of Quality (CQ), and Material Safety Data Sheet (MSDS) — meeting factory audit requirements.
Delivery to Industrial Parks: VSIP Industrial Park (Binh Duong), Nhon Trach Industrial Park (Dong Nai), Amata Industrial Park (Bien Hoa).
Extensive warehouse network: Ba Ria – Vung Tau, Dong Nai, Binh Duong, Da Nang, Can Tho and Bac Ninh — ensuring stable inventory and no stockouts.
QCVN compliance: Liquid PAC (Polyaluminium Chloride) meets QCVN 01:2009/BYT for potable water. Liquid PAC (Polyaluminium Chloride) for wastewater meets QCVN 40:2025/BTNMT (superseding QCVN 40:2011, effective Sept 1, 2025).
Technical support: Dosage consulting, chemical dosing point design, and Jar Test assistance.

Contact Us to Purchase Liquid PAC (Polyaluminium Chloride) with Delivery to Industrial Parks

📞 Hotline: 0979 891 929
📩 Email: [email protected]
🌐 Website: hoachatlocthien.com
🚚 Delivery: VSIP I and VSIP II Industrial Parks (Binh Duong), Nhon Trach 1-5 Industrial Parks (Dong Nai), Amata Industrial Park (Bien Hoa).

Frequently Asked Questions About Liquid PAC (Polyaluminium Chloride)

What is liquid PAC (Polyaluminium Chloride)? What is the Al₂O₃ percentage?

Liquid PAC (Polyaluminium Chloride)

Aluminum Chloride (CAS 1327-41-9) is a aluminum-based coagulation solution with an Al₂O₃ content ranging from 10% to 17%. Its liquid form allows for direct metering without generating dust, making it suitable for automated production lines in water treatment plants and Wastewater Treatment facilities.

What is the difference between liquid PAC (Polyaluminium Chloride) 10% and 17%? How are they used for turbid water?

Liquid PAC (Polyaluminium Chloride) 10% is suitable for water with low to moderate turbidity (10–100 NTU), at a dosage of 1–5 mg/L. Liquid PAC (Polyaluminium Chloride) 17% is used for highly turbid water (100–500 NTU) or industrial wastewater, at a dosage of 5–15 mg/L. A higher Al₂O₃ concentration means less chemical is needed to achieve the same coagulation effect.

Liquid PAC (Polyaluminium Chloride) vs. Powdered PAC (Polyaluminium Chloride) — Advantages and Disadvantages in Water Treatment Plants?

Liquid PAC advantages: direct dosing, dust-free, easy to automate, and safe for workers. Disadvantages: lower concentration than powdered PAC, so larger storage tanks are required. Powdered PAC advantages: high concentration (28–31%), saves storage space. Disadvantages: Must be pre-mixed, generates dust, and poses an inhalation risk. For automated water treatment plants, liquid PAC (Polyaluminium Chloride) is the optimal choice.

What is the recommended dosage of liquid PAC (Polyaluminium Chloride) for turbid water at 50–200 NTU?

For turbid water at 50–200 NTU, the recommended dosage of liquid PAC (Polyaluminium Chloride) is: 3–8 mg/L (liquid PAC (Polyaluminium Chloride) 10%) or 2–5 mg/L (liquid PAC (Polyaluminium Chloride) 17%). A Jar Test should be conducted to determine the optimal dosage for each water source. Loc Thien offers Jar Tests for purchases of 200 kg or more per month.

Does Loc Thien’s liquid PAC (Polyaluminium Chloride) comply with the QCVN 01:2009/BYT standard for potable water?

Yes. Loc Thien’s liquid PAC (Polyaluminium Chloride) meets the QCVN 01:2009/BYT standard for potable water applications. Each shipment includes a CoA (Certificate of Analysis), CO (Certificate of Origin), CQ (Certificate of Quality), and MSDS (Material Safety Data Sheet). Customers may request these documents prior to placing an order.

Can I purchase liquid PAC (Polyaluminium Chloride) for delivery to the VSIP, Nhon Trach, and Amata industrial parks?

Loc Thien delivers liquid PAC (Polyaluminium Chloride) to the VSIP I and VSIP II Industrial Parks (Binh Duong), Nhon Trach Industrial Zones 1, 2, 3, and 5 (Dong Nai), Amata Bien Hoa Industrial Zone, Long Binh Industrial Zone (Dong Nai), and industrial zones in Ho Chi Minh City. Order by 10 a.m. for delivery. Hotline: 0979 891 929.

Technical Engineering Guides, Specific Gravity Tables & Core Flagship Products

Core Flagship Products in Stock Across 6 Vietnam IP Warehouses (5–30-Ton Tankers & IBC/Bags): PAC 17% Liquid Polyaluminium Chloride · Liquid Poly Aluminium Chloride 10% & 17% (Liquid PAC) · Poly Aluminium Chloride Powder 30%–31% (PAC Powder).

In-Depth Engineering Guides, Specific Gravity Tables & ETP Dosing Protocols:

2026 Vietnam Chemical Law Compliance (Law No. 69/2025/QH15 & Decrees 24–26/2026/NĐ-CP) & EPE Customs Support

Under Vietnam's regulatory framework effective in 2026—including the Law on Chemicals No. 69/2025/QH15, Decree 24/2026/NĐ-CP (Industrial Precursor Management), Decree 25/2026/NĐ-CP, Decree 26/2026/NĐ-CP, and Circular 01/2026/TT-BCT—FDI enterprises and Export Processing Enterprises (EPEs) require strict legal traceability across their chemical supply chain. Loc Thien guarantees full compliance on every delivery:

2026 Regulatory & B2B Scope Governing Standard Loc Thien Chemical Execution Commitment
Group 2 Industrial Precursor Control Law 69/2025/QH15 & Decree 24/2026/NĐ-CP Fully licensed to trade Group 2 precursors (H2SO4, HCl, HNO3, H2O2, Toluene) with compliant purchase-sale control slips and electronic lot traceability.
16-Section GHS SDS & Batch COA Decree 26/2026/NĐ-CP & Circular 01/2026/TT-BCT Every shipment includes a batch-matched Certificate of Analysis (COA) and bilingual 16-section GHS Safety Data Sheet (SDS) for EHS audits.
Licensed 5–30-Ton Hazmat Tanker Fleet Decree 25/2026/NĐ-CP & Dangerous Goods Transport Rules Dedicated 5–30-ton tankers (3,000+ MT/month capacity) with valid hazmat transport permits, FRP/PE/SS linings, certified drivers, and onboard spill kits.
EPE On-Spot Customs & 15-Minute Quote SLA Vietnam EPE Customs Rules & Loc Thien SLA Full support for on-spot import/export customs declarations (0% VAT) for EPE factories. Technical quotation within 15 minutes; delivery within 4 hours in inner HCMC, 24–48 hours across Southern & Mekong Delta IPs, and 2–3 days in Northern & Central Vietnam.

Contact hotline 0979 891 929 or email [email protected] for detailed delivery procedures, sample COA/SDS documentation, and a technical quotation within 15 minutes.

WeChat B2B

Connect via WeChat B2B

Loc Thien Chemical — Direct Manufacturer & Industrial Chemical Supplier

Loc Thien Chemical Official WeChat B2B QR Code 0979891929

Scan QR code with WeChat on your phone

WeChat ID 0979891929

Tap the copy button above, then open WeChat and paste ID into Search to connect.

Direct Technical & Bulk Quotation Hotline: 📞 0979 891 929