H2O2 35% Food Grade INTEROX FCC 35 — Solvay Thailand
H₂O₂ 35% food grade INTEROX FCC 35 (Solvay Thailand) — CAS 7722-84-1, UN 2014. FCC (Food Chemical Codex): As ≤0.5 ppm, Fe ≤0.5 ppm, Pb ≤4.0 ppm. COA batch P69260203: 35.5%. Direct import. ☎ 0979 891 929.
H₂O₂ 35% food grade INTEROX FCC 35 — hydrogen peroxide meeting Food Chemical Codex (FCC) standards, Solvay Peroxythai Limited, Map Ta Phut, Rayong, Thailand. CAS 7722-84-1, UN 2014 (Class 5.1 + 8, PG II). Actual concentration 35.5% w/w (COA batch P69260203), density 1.12 g/cm³ @ 20°C.
FCC 35 differs from industrial H₂O₂ in impurity thresholds: As ≤0.5 ppm (4× cleaner than industrial ≤2.0 ppm), Fe ≤0.5 ppm (2× cleaner), Pb ≤4.0 ppm (2.5× cleaner). Meets food, pharmaceutical and cosmetic sterilization requirements — certified according to FCC and 21 CFR 184.1366.
Lộc Thiên directly imports — supplies batch-specific COA and MSDS per Circular 01/2026/TT-BCT. Quotation within 15 minutes. Hotline 0979 891 929.
- CAS 7722-84-1 — UN 2014 (Class 5.1 + 8, PG II)
- Content 35.5% w/w (COA batch P69260203) — spec ≥35.0%
- Density 1.12 g/cm³ @ 20°C — lighter than H₂O₂ 50% (1.12 vs 1.20)
- FCC certified: As ≤0.5 ppm, Fe ≤0.5 ppm, Pb ≤4.0 ppm
- Origin: Solvay Peroxythai Limited, Thailand — direct import
| Parameter | Specification | Notes |
|---|---|---|
| Trade name | INTEROX FCC 35 (Solvay) | Per MSDS — imported from Thailand |
| Formula | H₂O₂ | Molar mass 34.01 g/mol |
| CAS | 7722-84-1 | — |
| UN Number | UN 2014 | Class 5.1 + 8, PG II |
| Assay (COA) | 35.5% w/w (batch P69260203) | Spec ≥35.0% — COA per lot |
| Density @ 20°C | 1.12 g/cm³ | Lighter than industrial H₂O₂ 50% (1.20) |
| Stability | 0.21 (spec ≤3.00) | Suitable for long-distance transport |
| Acidity (H₂SO₄) | 0.01% (spec ≤0.03%) | Very low — reduced corrosion risk |
| As | <0.1 mg/kg | FCC spec: ≤0.5 mg/kg |
| Fe | <0.0 mg/kg | FCC spec: ≤0.5 mg/kg |
| Pb | <0.0 mg/kg | FCC spec: ≤4.0 mg/kg |
| Phosphate | ≤50.0 mg/kg | FCC spec |
| Non-volatile residue | ≤60.0 mg/kg | FCC spec |
| Sn | ≤10.0 mg/kg | FCC spec |
| Origin | Solvay Thailand — direct import | — |
| Packaging | 30kg HDPE drum / 5–30 ton tanker | — |
Usage notes
Strong oxidizer — use PPE and store per MSDS. Verify concentration on COA before dilution. Do not mix with heavy metals, strong alkalis, or organic substances. Dilute with purified water for food applications.
💬 Technical Specialist Phan Cẩm Thùy (15 years experience): "Solvay Thailand FCC 35% H2O2 is the optimal choice for food plants requiring international certification. Heavy metals 2–4 times lower than industrial grade, especially As <0.1 mg/kg — safe for direct food contact applications. Always request the batch COA to confirm actual concentration."
📖 See also: H2O2 Food Grade FCC 35% vs Industrial 50% — Detailed Comparison | Applications of H2O2 35% in Food Processing