PAC 31% (Poly Aluminium Chloride) Powder — Real COA, Delivery to Industrial Parks

Key Technical Summary: PAC 31% powder — real COA Al₂O₃ 28.59%. 3 sources: Viet Tri/Tenor/India. Quote in 15 min, nationwide delivery. Call 0979 891 929.
Table of contents
| Parameter | Value | Method |
|---|---|---|
| Al₂O₃ content | 28.59% | TCVN |
| Basicity | 40.12% | TCVN |
| Cl | 35.73% | TCVN |
| SO₄ | 0.81% | TCVN |
| pH (5% solution) | 3.58 | TCVN |
| Bulk density | 0.79 g/mL | TCVN |
| Insoluble impurities | 0.14% | TCVN |
| Color | White to pale yellow | Visual |
| Result | PASS | — |
| CAS | 1327-41-9 | — |
| Formula | [Al₂(OH)ₙCl₆₋ₙ]ₘ | — |
| Packing | 25 kg/bag | — |
All data above is real COA from the batch tested by Loc Thien QC Department. Each batch may vary ±1% depending on production conditions. Customers receive batch-specific COA upon purchase.
Differentiating PAC Viet Tri, PAC China (Tenor) and PAC India
The PAC 31% market in Vietnam mainly comes from 3 sources: PAC Viet Tri domestically produced, PAC Tenor imported from China, and PAC India. Below is a comparison table based on actual COA data from batches Loc Thien is currently supplying. The choice of source depends on budget, quality requirements and specific treatment conditions of each plant.
| Criterion | PAC Viet Tri 31% | PAC Tenor (China) | PAC India |
|---|---|---|---|
| Origin | Vietnam | China | India |
| Al₂O₃ | 28–31% | 28–30% | 28–30% |
| Basicity | 40–60% | 40–70% | 40–50% |
| pH (1% solution) | 3.5–4.5 | 3.5–4.5 | 3.5–5.0 |
| Color | Off-white | Pale yellow | White |
| Price | Medium | Lowest | Highest |
| Quality consistency | High | Medium | High |
| Stock at Loc Thien | Continuous | Continuous | Made-to-order |
| Delivery time | 24–48 hours to Southern IPs | 24–48 hours to Southern IPs | Advance order |
PAC Viet Tri is the most balanced choice with stable quality, reasonable price and always available at Loc Thien’s warehouses. PAC Tenor China suits plants optimizing costs. PAC India is for organizations requiring clear origin with the highest quality. Loc Thien supplies all 3 sources, so customers can proactively choose based on their needs.
PAC 31% Applications in Water Treatment
PAC 31% powder is used in drinking water, wastewater, swimming pool and aquaculture treatment. For drinking water treatment, PAC 31% removes turbidity and organic matter at 10–30 mg/L, reducing sludge compared to alum. In industrial wastewater (textile dyeing, paper, seafood processing, food), PAC 31% achieves high coagulation efficiency at 20–60 mg/L, reducing COD by 65–80%. For swimming pool water, PAC 31% is used periodically at 5–10 mg/L combined with Javen for disinfection. In aquaculture ponds, dosage of 2–5 kg/1,000 m³ helps settle silt and heavy metals. Compared to PAC 17% liquid form, PAC 31% powder has double the content, saving transportation and storage costs. Combining with FeCl3 in wastewater treatment improves coagulation efficiency at low pH.
Figure: On-site chemical dosing, storage tank operation, and batch COA inspection — Source: Loc Thien Chemical.
PAC 31% Dosage and Jar-test Procedure
PAC 31% dosage depends on turbidity, pH and source water properties. The table below provides reference dosages for common applications. Loc Thien recommends performing a jar-test before full-scale dosing to optimize performance and cost. Standard jar-test procedure: prepare PAC 31% as a 5–10% solution, add to 6 water beakers with increasing doses, rapid mix at 200 rpm for 2 minutes, slow mix at 40 rpm for 15 minutes, settle for 20 minutes and measure residual turbidity. The optimal dose is the one giving the lowest turbidity with maximum floc formation.
| Application | Reference dosage (mg/L) | Optimal pH | Notes |
|---|---|---|---|
| Drinking water supply | 10–30 | 6.5–8.5 | Reduce turbidity < 1 NTU |
| Textile dyeing wastewater | 30–60 | 6.0–8.0 | Reduce COD 65–75% |
| Seafood processing wastewater | 25–50 | 6.0–8.5 | Reduce COD, TSS |
| Swimming pool water | 5–10 | 7.0–7.8 | Weekly periodic treatment |
| Aquaculture ponds | 2–5 kg/1,000 m³ | 6.5–8.5 | Periodic treatment |
| Industrial park wastewater | 20–60 | 6.0–9.0 | Perform jar-test first |
Combining PAC 31% with PAC 10% liquid and NaOH helps flexibly adjust pH in continuous treatment systems. For wastewater sources with low pH, raise pH to 6.5–7.5 before dosing PAC using NaOH or lime.
Legal Documentation per Batch
Each batch comes with full legal documentation: real batch-specific COA (Certificate of Analysis), MSDS (Material Safety Data Sheet) and framework contract. Loc Thien’s quality control process consists of 3 steps: incoming inspection at warehouse by Phan Cam Thuy, periodic in-storage inspection, and pre-dispatch inspection approved by Vo Thi Nhu Hoa. CAS 1327-41-9 of PAC 31% is classified by the Ministry of Industry and Trade as a general industrial chemical, not on the list of precursors or restricted chemicals, facilitating purchase, sale and transport procedures.
Why Choose Loc Thien Chemical for PAC 31%?
Loc Thien operates 6 strategic warehouses nationwide (Ba Ria – Vung Tau, Dong Nai, Binh Duong, Da Nang, Can Tho and Bac Ninh) with a fleet of tanker trucks of 5–30 tons, ensuring delivery to industrial parks in the southern region. The key difference is quality: each batch of PAC 31% comes with a real COA with full specifications such as Al₂O₃ 28.59%, basicity 40.12% — no blending, no hidden numbers. Loc Thien maintains direct import relationships with factories in Viet Tri, China and India, enabling competitive pricing and stable supply during peak seasons. The technical team supports on-site jar-testing at customer plants, optimizing dosage from the very first batch. With over 10 years serving plants and industrial parks nationwide, Loc Thien is a reliable water treatment chemical supply partner.
PAC 31% Pricing & How to Get a Quote
PAC 31% price depends on origin (Viet Tri, Tenor China or India), order quantity and import timing. Loc Thien publishes transparent pricing per batch COA, with no fixed listed price as raw material costs fluctuate with world markets. To receive the fastest PAC 31% quote, customers please call hotline 0979 891 929 or send a request to [email protected] with the following information: desired origin, quantity (kg/month), delivery location. A quote is sent within 15 minutes along with a reference COA. For large orders (over 5 tons), Loc Thien offers volume-based discounts, with delivery per our shipping policy.
Technical Support & B2B Procurement Hotline
Loc Thien Chemical specializes in direct manufacturing of FeCl₂ / FeCl₃ and direct industrial supply of basic chemicals (NaOH, HCl, H₂SO₄, PAC, NaOCl, H₂O₂, FeSO₄) with direct B2B pricing and dedicated 5–30-ton tanker delivery across Vietnam.
- Hotline / Zalo: +84 979 891 929
- Official Email: [email protected]
- Direct Manufacturer: Ferrous Chloride (FeCl₂ 30%) & Ferric Chloride (FeCl₃ 38–40%)
- Primary Supplier: NaOH 32%/45%/50%/99%, HCl 32%, H₂SO₄ 98%, PAC 30–31%, NaOCl 10–12%, H₂O₂ 35%/50%
- Compliance & Quality: FeCl₂ ZDHC MRSL v3.1 test report (Smart testing, 5 substance groups, TUV Rheinland Vietnam), ISO 9001:2015, Quatest 3, Full COA & GHS SDS
Frequently Asked Questions about PAC 31%
Does PAC 31% dissolve completely in water?
Yes, PAC 31% powder dissolves completely in water, forming a clear solution. To speed up dissolution, dilute at a ratio of 5–10% (5–10 kg powder per 100 L water), stir for 5–10 minutes before dosing into the system.
How to distinguish PAC 31% powder from liquid PAC?
PAC 31% powder has 2–3 times higher Al₂O₃ content than liquid PAC (PAC 10% liquid has only 10% Al₂O₃). Powder PAC saves on transportation and storage costs but requires preparation time. Liquid PAC is more convenient for direct dosing systems.
Should I use PAC 31% or alum?
PAC 31% is superior to alum in 3 aspects: produces larger flocs, works well at low temperatures, and reduces sludge by 40–50%. Meanwhile, alum has a lower purchase price but higher sludge treatment costs.
Can PAC 31% be used together with FeCl3?
PAC 31% and FeCl3 can be used alternately or in combination depending on wastewater characteristics. FeCl3 (What is FeCl3?) is effective at low pH (4.0–6.0), while PAC 31% works well at neutral to alkaline pH (6.0–9.0). The two chemicals complement each other in systems with fluctuating pH.
Does PAC 31% require a coagulant aid?
For high-turbidity source water or fast-settling systems, combining PAC 31% with coagulant polymer (anionic or non-ionic) helps form larger flocs, faster settling, and reduces PAC consumption by 10–20%.
How to receive the real COA for the batch?
COA is sent with each dispatched batch. Customers can request COA before delivery via hotline. Each COA clearly states the production date, analysis results and approver.
What is the delivery time for PAC 31%?
Delivery to industrial parks in Ho Chi Minh City, Dong Nai, Binh Duong. Central and Northern regions: 24–48 hours. Call hotline 0979 891 929 to confirm specific delivery schedule per warehouse.
What is the shelf life of PAC 31%?
Shelf life is 24 months from production date, stored in a dry place away from direct sunlight. The product may absorb slight moisture but remains effective if still within shelf life and not hardened into lumps.
Where to Buy Reputable PAC 31% in Vietnam?
Loc Thien Chemical supplies bulk quantities of quality PAC 31% with real batch-specific COA and delivery to industrial parks. Customers can order directly via hotline or email for free technical consultation and PAC 31% pricing per origin: Viet Tri, Tenor China or India. Trial orders of 25–100 kg are always available for dispatch from the nearest warehouse.
- Hotline: 0979 891 929 (call now for a quote within 15 minutes)
- Email: [email protected]
- Address: 452/6B Tinh Lo 10 (Provincial Road 10), Binh Tri Dong Ward, Ho Chi Minh City
- Warehouses: Ba Ria – Vung Tau, Dong Nai, Binh Duong, Da Nang, Can Tho and Bac Ninh
- Tax code: 0313650856
- Delivery time: 24–48 hours to southern industrial parks, 2–3 days to Northern and Central Vietnam
- Website: https://hoachatlocthien.com
🛒 Need PAC 31%? Get a quote for PAC 31% powder — Batch COA/MSDS, delivered to industrial parks nationwide. Hotline 0979 891 929.
Industrial Field Operation & Batch Quality Verification
1. Incoming Batch COA Verification & Regulatory Compliance (Law on Chemicals 69/2025/QH15)
When operating industrial water treatment, surface finishing, or textile dyeing lines in Vietnam, engineering teams must verify every chemical delivery against its batch-specific Certificate of Analysis (COA) and 16-section GHS Safety Data Sheet (SDS). Under the Vietnam Law on Chemicals No. 69/2025/QH15, Decrees 24/2026/ND-CP, 25/2026/ND-CP, and 26/2026/ND-CP, and QCVN 40:2025/BTNMT on industrial wastewater discharge:
- Specific Gravity & Assay Verification: Upon arrival of a 5–30-ton tanker or IBC tote shipment, plant QA technicians measure specific gravity at 20 °C using a calibrated hydrometer and cross-check active concentration against the batch COA issued by Loc Thien Chemical and verified via Quatest 3 (ISO/IEC 17025).
- Impurity & Heavy Metal Control: Trace heavy metals (Fe, Pb, As, Hg, Cd, Cr⁶⁺) and insoluble matter are strictly controlled to prevent catalyst poisoning in Fenton reactors, membrane fouling in RO/UF systems, or shade deviations in reactive textile dyeing.
- ZDHC MRSL v3.1 Level 1 Portfolio Boundary: For export-oriented textile and footwear FDI factories, Loc Thien Chemical maintains official ZDHC MRSL v3.1 Conformance Level 1 documentation for exactly 9 core products: four products certified by TUV SUD Product Service GmbH (
NaOH,H2O2,Na2SO4,Na2CO3) and five products verified via Conformance Summary Report (CSR) and Analytical Test Report by TUV Rheinland Vietnam (H2SO4,FeCl2,HCl,Javel/NaOCl,PAC 31%).
| Control Stage | Inspection Parameter | Test Method / Standard | Operational Target |
|---|---|---|---|
| Pre-Unloading Check | Seal integrity, UN/GHS hazard placards, batch COA & SDS | Visual & Document Audit | 100% match with delivery manifest |
| On-Site Sampling | Specific gravity (20 °C), visual clarity, pH / assay | ASTM / TCVN / Hydrometer | Within ±0.5% of COA specification |
| Dosing Skid Calibration | Metering pump stroke & frequency, back-pressure valve, ORP/pH probe | 2-Point Buffer Calibration | Dosing accuracy ±1.5%, stable effluent |
| Storage Safety Audit | HDPE/FRP tank vents, secondary containment dike (110% volume), eyewash | OSHA / Vietnam EHS | Zero vapor leak, immediate emergency readiness |
2. Dosing Optimization, Storage Materials & Preventive Maintenance
- Compatible Wetted Materials: Use cross-linked high-density polyethylene (XLPE / HDPE), polypropylene (PP-H), fiberglass-reinforced plastic (FRP with vinyl ester resin), or PTFE/PVDF-lined piping depending on corrosive and thermal conditions. Avoid unlined carbon steel or incompatible elastomers.
- Automated Dosing Control: Integrate diaphragm metering pumps with real-time pH, ORP (mV), turbidity, or conductivity sensors. Always perform a 5-beaker Jar Test whenever raw water COD, TSS, or alkalinity shifts by more than 15%.
- Secondary Containment & PPE: Storage tanks must sit inside an acid/alkali-resistant bund wall holding at least 110% of the largest tank volume. Operators handling unloading hoses must wear splash-proof chemical goggles, acid/alkali-resistant nitrile or neoprene gloves, face shields, and emergency respirators.
3. Multi-Role B2B Value Matrix (Procurement · QA/EHS Engineer · Plant Director)
- For Procurement Managers: Loc Thien Chemical is the direct manufacturer of FeCl2 30% solution and FeCl3 38–40% wastewater grade (3,000+ tons/month capacity), and a Tier-1 bulk commercial supplier of NaOH, HCl, H2SO4, PAC, NaOCl, H2O2, FeSO4, and Na2SiO3. Pricing is transparently structured around 5 technical cost drivers (active assay, packaging format, delivery distance from our 6 warehouses, order volume, and scheduled contract cadence) with a 15-minute technical quotation SLA.
- For Environmental & Process Engineers: Full technical support for Jar Test optimization, stoichiometry calculation, sludge minimization, and QCVN 40:2025/BTNMT compliance auditing.
- For FDI Plant Directors: Guaranteed supply continuity via 6 regional warehouses (Ba Ria - Vung Tau, Dong Nai, Binh Duong, Da Nang, Can Tho, Bac Ninh) and a dedicated 5–30-ton tanker fleet (4 hours in inner HCMC, 24–48 hours across Southern & Mekong Industrial Parks, 2–3 days in Northern & Central Vietnam).
4. Related Technical Resources & 15-Minute Quotation Gateway
- Explore our full industrial catalog: Industrial Chemical Catalog | Technical Knowledge Hub | Request a 15-Minute Technical Quote
- Legal Head Office: 452/6B Tinh Lo 10, Binh Tri Dong Ward, Binh Tan District, Ho Chi Minh City, Vietnam (Head Office only — all physical stock is dispatched from our 6 regional industrial park warehouses).
- 24/7 Technical Hotline: 0979 891 929 (Please contact hotline 0979 891 929 for detailed delivery procedures) | Official Email: [email protected]