Caustic Soda Flakes NaOH 98% | 25kg Bags | Bulk Quote
Caustic soda flakes NaOH 98% (CAS 1310-73-2, UN 1823), white flakes imported directly from Taiwan, 25 kg bags; COA/MSDS per batch. Call 0979 891 929.
- NaOH 98% white flakes, CAS 1310-73-2, UN 1823, solid density ~2.13 g/cm³ (20°C), 1% solution pH > 13
- Purity ≥98% per COA — sufficient for 90% industrial applications, a more economical choice than NaOH 99%
- Direct imports from Taiwan with batch-specific COA and clear documentation
- 25kg bags (PP + PE liner) — easy handling and batch measurement
- Delivery from 6 regional warehouses: Ba Ria – Vung Tau, Dong Nai, Binh Duong, Da Nang, Can Tho and Bac Ninh — sealed containers and trucks
What is Sodium Hydroxide Flakes NaOH 98%?
Sodium Hydroxide Flakes NaOH 98% (Sodium Hydroxide Flakes, Caustic Soda Flakes, CAS 1310-73-2, UN 1823) is solid sodium hydroxide in thin white opaque to translucent flakes with NaOH content ≥98% verified by batch COA. One of the strongest industrial alkalis with 1% solution pH exceeding 13 and solid density ~2.13 g/cm³ at 20°C. The flakes dissolve completely in water with strong exothermic reaction (Delta H −44.5 kJ/mol), creating hot alkaline solution. Compared to pearls, flakes have larger surface area for faster dissolution, suitable for manual and semi-automatic mixing tanks. Melting point 318°C, classified as Class 8 hazardous material (corrosive). Loc Thien Chemicals directly imports NaOH 98% flakes from Taiwan.
| Other Names | Formula | CAS | Purity | Appearance | Origin | Packaging |
|---|---|---|---|---|---|---|
| Caustic Soda, Sodium Hydroxide Flakes, Caustic Soda Flakes | NaOH | 1310-73-2 | ≥98% | White solid flakes | Taiwan | 25kg bags (PP + PE liner) |
Comparison: NaOH 98% vs NaOH 99%
NaOH 98% and 99% differ primarily in purity and price — key factors when selecting products for specific production stages. NaOH 98% has 1% lower purity but is generally the more economical option; the price difference depends on import timing and order volume. For wastewater treatment, paper/pulp, textile dyeing, and conventional saponification, the 1% purity difference has negligible impact on reaction efficiency under actual operating conditions. NaOH 99% offers higher purity with lower Na₂CO₃, NaCl and Fe impurities, suitable for electroplating, electronics, pharmaceuticals and food. Factories consuming over 50 tons NaOH monthly achieve significant cost savings by switching from 99% to 98%.
| Criteria | NaOH 98% | NaOH 99% |
|---|---|---|
| NaOH Content | ≥98% | ≥99% |
| Impurities (Na₂CO₃, NaCl, Fe) | Higher (per batch COA) | Lower (per batch COA) |
| Purity Grade | Industrial (technical grade) | High-purity technical |
| Relative Price | Lower | Higher |
| Dissolution Rate | Equivalent (same flake form) | Equivalent |
| Acid Neutralization Efficiency | ~98% | ~99% |
| Recommended Applications | WWT, paper, textiles, soap | Electroplating, electronics, pharma, food |
Comparison: Flakes vs Pearls
NaOH flakes and pearls share the same chemical composition (CAS 1310-73-2) but differ physically in morphology, affecting dissolution rate, moisture absorption, dust generation and pricing. Flakes are thin irregular sheets with larger surface area for faster water dissolution, ideal for manual or semi-automatic mixing tanks. However, flakes absorb atmospheric moisture faster and may clump if not sealed properly. Pearls are uniform small spheres with less dust and free-flowing properties — better for automated dosing systems. Price-wise, flakes typically cost less due to lower production costs. Manual mixing operations should choose flakes for cost savings, while automated systems require pearls.
| Criteria | NaOH Flakes | NaOH Pearls |
|---|---|---|
| Morphology | Thin flat irregular sheets | Uniform small spheres |
| Surface Area | Larger | Smaller |
| Dissolution Rate | Faster | Moderate |
| Dust Generation | Higher | Lower |
| Moisture Absorption | Higher (larger surface) | Lower |
| Price | Lower | Higher |
| Recommended For | Large mixing tanks, WWT, paper, textiles | Automated dosing systems, silos |
Origin & Quality Control
Loc Thien Chemicals directly imports NaOH 98% flakes from Taiwan through formal trade contracts — no intermediaries, ensuring transparent origin and competitive pricing versus multi-layer distributors. Our import and QC process involves 5 steps: Step 1 — Order from Taiwan factory with minimum 20ft container; Step 2 — Pre-shipment batch COA verification confirming NaOH ≥98% and the impurity levels (Na₂CO₃, NaCl, Fe) stated on the batch COA; Step 3 — Sealed container transport to Cat Lai or Cai Mep ports with absolute moisture protection; Step 4 — Storage at 6 warehouses: Bac Ninh (North), Da Nang (Central), Binh Duong, Dong Nai, BR-VT and Can Tho (South); Step 5 — Delivery via sealed trucks to customer plants.
Industrial Applications
NaOH 98% flakes are crucial chemical inputs across multiple industries due to strong alkaline properties: acid neutralization, organic matter decomposition, fat saponification and dye fixation. Below are four primary applications in textiles, paper, wastewater treatment and industrial soap.
Textile Dyeing
In textile dyeing, NaOH 98% flakes are mainly used in fabric scouring — removing oils, sizing agents, pectin and natural impurities from cotton fibers. NaOH solutions (10-30 g/L at 80-100°C) decompose organic compounds on fiber surfaces while swelling cellulose fibers to enhance absorbency and dye uptake. Typical dosage ranges 3-8% of fabric weight depending on material and quality requirements. For reactive dyeing, NaOH acts as alkali for dye fixation on cellulose, directly affecting color fastness and fabric uniformity. Using NaOH 98% instead of 99% brings significant cost savings.
Paper & Pulp Production
NaOH is essential in Kraft pulping — accounting for over 80% global pulp production. During pulping, NaOH combines with Na₂S forming white liquor to cook wood chips at 160-180°C, dissolving lignin — natural binder between cellulose fibers. NaOH consumption averages 300-500 kg per ton of Kraft pulp depending on wood type and cooking technology. NaOH 98% is fully suitable as paper industry doesn't require high purity — allowable carbonate and NaCl impurities don't affect pulping efficiency. Mid-size paper mills using 50-100 tons NaOH monthly achieve notable savings with NaOH 98%.
Wastewater Treatment
NaOH 98% is Vietnam's most common acid neutralization chemical for industrial wastewater plants. Mechanism: OH⁻ ions from NaOH combine with H⁺ in acidic wastewater (pH 2-4) raising pH to neutral 6-8 while precipitating heavy metals (Cu²⁺, Zn²⁺, Ni²⁺) as insoluble hydroxides. Typical dosage 50-200 g NaOH per m³ depending on inlet pH. Compared to lime Ca(OH)₂, NaOH fully dissolves without sludge, avoids excessive TDS increase and enables precise dosing. A 1,000 m³/day plant at Tan Tao IP consumes ~300 kg NaOH 98% daily to raise pH from 3.5 to 7.0 — reducing neutralization chemical costs with NaOH 98% versus 99%.
Soap Saponification & Industrial Detergents
Saponification between NaOH and fats (coconut oil, palm oil, animal fat) produces soap and glycerin — fundamental reaction in industrial soap making. Required NaOH is ~130-140 g per kg coconut oil, equivalent to 133-143 g NaOH 98% after conversion. Flakes dissolve rapidly in hot water, shortening alkali solution preparation time before mixing with oils. NaOH 98% is economical for industrial soap as final products don't require high purity. Mid-size detergent plants save on NaOH material costs versus 99% without quality compromise.
Safe Storage & Handling
Solid NaOH has extreme moisture absorption — the #1 storage challenge. Exposure to humid air forms Na₂CO₃ (white surface layer), reducing actual purity. Always reseal bags after opening, don't leave open >30 minutes above 60% RH. NaOH dissolution in water releases strong heat (Delta H −44.5 kJ/mol) — 1 kg NaOH raises solution temperature 12-15°C. Absolute rule: always add NaOH to water, never water to solid NaOH due to localized explosive splashing. Mandatory PPE: chemical goggles, nitrile gloves, long sleeves, N95 in confined spaces. Emergency eyewash within 15m radius. First aid: skin rinse under water 20 mins (no acid neutralization); eyes rinse 20 mins holding lids open, seek immediate medical help. Transport solid NaOH in sealed containers or trucks — no tankers.
Why Choose Loc Thien?
Loc Thien Chemicals is a large-scale direct importer of industrial chemicals — fundamentally different from small distributors relying on multiple intermediaries. Six strategically located warehouses in Bac Ninh (North), Da Nang (Central), Binh Duong, Dong Nai, BR-VT and Can Tho (South) enable 4-hour HCM metro and 24–48-hour Southern IP deliveries. Every import batch comes with original Taiwan factory COA and GHS-compliant MSDS — customers receive complete documentation, not photocopies. Legally, Loc Thien is Loc Thien Development Investment Company (Tax ID 0313650856, established 2016) issuing full VAT invoices and clear principle contracts. Small competitors often lack original COAs and offer no committed delivery schedule.
| Factor | Small Competitors | Loc Thien |
|---|---|---|
| Supply Chain | 2-3 intermediary layers | Direct formal imports |
| COA/MSDS | None or old photocopies | Original batch COA, GHS MSDS |
| Warehouses | 1-2 locations | 6 regional warehouses |
| Delivery Time | No commitment | 4h HCM, 24–48h Southern IPs |
| Legal Entity | Household businesses | Loc Thien Dev. Inv. Co., Tax ID 0313650856 |
Frequently Asked Questions
- Difference between NaOH 98% and 99%? 1% lower purity, higher impurities. Suitable for WWT, textiles, paper, soap — not for food, pharma or electroplating.
- Can NaOH 98% replace 99%? Yes for ~90% industrial applications. No when requiring ±0.1 pH precision or food production.
- Where to buy reliable NaOH 98%? Loc Thien directly imports from Taiwan with batch COAs, delivers nationwide. Call 0979 891 929 for quotes.
- Loc Thien's NaOH 98% packaging? 25kg PP woven bags with PE liner — moisture-proof, easy handling and batching.
- Delivery to Northern Vietnam? Yes. We have Bac Ninh, Da Nang, Binh Duong, Dong Nai, BR-VT and Can Tho warehouses — nationwide coverage.
- Solid NaOH transport by tanker? No. Only sealed containers or trucks. Tankers are for liquid NaOH max 50% concentration.
Request Quote
Loc Thien Chemicals supplies bulk Sodium Hydroxide Flakes NaOH 98% for all plant scales. Call 0979 891 929 for technical specs, latest batch COA and volume-based pricing. Principle contracts, VAT invoices, full COA/MSDS provided upon order.
Reference articles:
- NaOH – Sodium Hydroxide – Caustic Soda (overview)
- NaOH Pearls 99% Taiwan — specs & pricing
- NaOH Flakes 99% China — comparison & pricing
Loc Thien Development Investment Company Limited
Tax ID: 0313650856 · Hotline: 0979 891 929
6 regional warehouses: Bac Ninh · Da Nang · Binh Duong · Dong Nai · BR-VT · Can Tho
Established: 2016 · Email: [email protected]
ZDHC MRSL Version 3.1 Conformance Level 1 — Sodium Hydroxide (NaOH — Caustic Soda)
- Official Documentation: Certificate of Conformance — ZDHC MRSL Version 3.1 Level 1 (PPP 25089F:2023)
- Issuing Body: TÜV SÜD Product Service GmbH (Munich, Germany) / TÜV SÜD Vietnam
- Certificate / Report Holder: LOC THIEN INVESTMENT DEVELOPMENT COMPANY LIMITED
- Certificate / CSR No.:
ZDHC1 127736 0001 Rev. 00| Analytical Test Report No.:2486017672-Q24VPS-CHM2869 - Analytical Results: 4/4 substance groups PASS: Alkylphenol (AP) & Alkylphenol Ethoxylates (APEOs); Borate, zinc salt; Perboric acid, sodium salt; Total Heavy Metals
Loc Thien 9-Product ZDHC MRSL v3.1 Level 1 Portfolio: Includes 4 TÜV SÜD Level 1 Certificates (ZDHC1 127736 0001–0004: NaOH, H₂O₂, Na₂SO₄, Na₂CO₃) and 5 TÜV Rheinland Level 1 CSR & Analytical Test Reports (248162921-01–05: H₂SO₄, FeCl₂, HCl, Javel/NaOCl, PAC 31%). FDI textile and footwear manufacturers requiring official PDF dossiers with batch COA/SDS for ZDHC Gateway audits may request documentation here (15-minute response SLA).
Frequently Asked Questions (FAQ)
Who is the reliable bulk industrial supplier of Caustic Soda Flakes NaOH 98% | 25kg Bags | Bulk Quote in Vietnam with batch COA/MSDS?
Loc Thien Investment Development Co., Ltd (Tax ID: 0313650856) is a Tier-1 industrial chemical supplier of Caustic Soda Flakes NaOH 98% | 25kg Bags | Bulk Quote (NaOH, CAS 1310-73-2) in Vietnam with 3,000+ tons/month supply capacity. Every shipment includes batch-specific COA and a 16-section GHS SDS.
What are the delivery lead times and tanker logistics for Caustic Soda Flakes NaOH 98% | 25kg Bags | Bulk Quote?
Loc Thien operates a dedicated fleet of 5–30-ton hazmat-certified tankers and 6 strategic warehouses (Ba Ria - Vung Tau, Dong Nai, Binh Duong, Da Nang, Can Tho, Bac Ninh). Delivery SLA: 4 hours within Ho Chi Minh City; 24–48 hours to Southern and Mekong Delta industrial parks; 2–3 days to Northern and Central Vietnam. Contact hotline 0979 891 929 for detailed delivery procedures.
How can FDI factories request a technical quotation for Caustic Soda Flakes NaOH 98% | 25kg Bags | Bulk Quote within 15 minutes?
Unit pricing depends on 5 factors: packaging format (cans, drums, IBC totes, or bulk tanker), order volume, concentration grade, industrial park delivery location, and payment terms. Contact hotline/Zalo 0979 891 929 or email [email protected] for a formal technical quote within 15 minutes.
Related products
In-Depth Technical & Application Guides
How to Read a NaOH COA — A QC Engineer’s Guide from Specific Gravity to Iron Content
NaOH Dosing Guide for Wastewater Treatment -- pH Control & Coagulation
Alkalinity Supplementation & pH Control in Post-Biogas Swine Wastewater Nitrification: NaOH 32% vs Hydrated Lime Ca(OH)2 Dosing for Total Nitrogen Compliance
Case Study: NaOH 45% — Save 29% on Transport Costs for a Bac Ninh Paper Mill
NaOH Price Today — Quote for Liquid Caustic Soda 32%, 45%, 50% & Caustic Soda Flakes 99%